317L Stainless Steel Round Tube 317l SS Tubing Pressure Rating Chart
video

317L Stainless Steel Round Tube 317l SS Tubing Pressure Rating Chart

Boiler tube applies to petroleum , chemical industry , electric power , boiler , high temperature resistant , low temperature resistant , corrosion resistant . The size can be made according to the customers requirements . High pressure boiler pipe applies to container , petrochemical and so on . Note : Generally , high pressure boiler pipe’s working pressure above 9.88Mpa and working temperature between 450 to 650 .
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of 317l stainless steel round tube 317l ss tubing pressure rating chart in China. If you're going to wholesale high quality 317l stainless steel round tube 317l ss tubing pressure rating chart made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

317L Stainless Steel Round Tube 317l SS Tubing Pressure Rating Chart

Description

OD: 6-630mm Thickness: 0.5-30mm
Surface: NO.1 Length: 6M
Type: Seamless Condition: Cold Rolled
High Light:

ss seamless pipes

,

astm stainless steel pipe

317L Stainless Steel Round Tube 317l SS Tubing Pressure Rating Chart

317L Stainless Steel

317L is a molybdenum bearing austenitic chromium nickel steel similar to type 316, except the alloy content in 317L is somewhat higher. It has a supperior corrosion resistance in special applications where it is desired to reduce contamination to a minimum. 317L was developed primarily to resist more effectively the attack of sulfurous acid compounds. Howerver, its proven ability to combat corrosion has widened its use considerably and is now being used for many other industrial applications. The low carbon content of 317L provides immunity to intergranular corrosion in applications where heavy cross sections cannot be annealed after welding or where low temperature stress relieving treatments are desired.

Availability - Stainless Steel 317L

Seamless Pipe 1/2" - 8"

Weld Pipe 1/2" - 12"

Butt-Weld Fittings 1/2" - 12"

Flanges 1/2" - 12"

 

Specifications - Stainless Steel 317L

ASTM A312, A403, A182
ASME SA312, SA403, SA182

 

Chemical Composition - Stainless Steel 317L

C Cr Mn Mo Ni P S Si
Max   Max Max   Max Max Max
0.08% 24% - 26% 2.0% 0.75% 19% - 22% 0.045% 0.03% 0.75%

 

Design Features - Stainless Steel 317L

A molybdenum bearing austenitic chromium nickel steel with an alloy content somewhat higher than the 316 grades.

Superior corrosion resistance in difficult environments.

Higher creep, stress-to-rupture and tensile strengths than other stainless steels.

Reduced intergranular precipitation of chromium carbides during welding and stress relieving as well as minimized possibility of corrosion failure from intergranular attack due to low carbon content.

Resistance to pitting and crevice corrosion making 317L a successful life-cost product in a variety of highly corrosive environments.

Typical Applications - Stainless Steel 317L

Flue gas desulfurization scrubber systems

Chemical and petro-chemical processing equipment

Pulp and paper plants

Food processing equipment

Textile equipment

Tensile Requirements - Stainless Steel 317L

Tensile Strength (KSI): 75

Yield Strength (KSI): 30

KSI can be converted to MPA (Megapascals) by multiplying by 6.895.

317L Stainless Steel Round Tube 317l SS Tubing Pressure Rating Chart 0

 

317L Stainless Steel Round Tube 317l SS Tubing Pressure Rating Chart 1