Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of 1.4568 1.4567 stainless steel pipe reducer in China. If you're going to wholesale high quality 1.4568 1.4567 stainless steel pipe reducer made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Stainless weld concentric reducers, as their name implies, reduce in diameter towards the center thus forming a conical cylinder. A concentric reducer is often used inline on a vertical flow application, or if laid horizontally, as an increaser. We do not recommend reducing in the horizontal as pooling may occur. In these cases, an eccentric reducer, which lays flat on one side is preferable. Concentric reducers have a lower chance of producing agitation like an end cap reducer may.


1.4568 1.4567 Stainless Steel Pipe Reducer Chemical Component
| C: | Mn: | Si: | P: | S: | Cr: | Ni: | Al: |
| <0.09 | <1.0 | <0.5 | <0.025 | <0.025 | 16.00 – 17.25 | 6.50 – 7.75 | 0.75 – 1.25 |
1.4568 1.4567 SS Pipe Reducer Mechanical Property
| Proof strength
Rp0.2 (MPa) |
Tensile strength
Rm (MPa) |
Impact energy
KV (J) |
Elongation at fracture
A (%) |
Reduction in cross section on fracture
Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
| 685 (≥) | 438 (≥) | 41 | 23 | 44 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 242 |
1.4568 Stainless steel from the group of age-hardened PH with the highest content of Chromium – 17% and Nickel – 7% in relation to PH of grades 15-5 and 17-4. It has excellent strength properties, high hardness and elasticity, good corrosion resistance and resistance to high temperatures and deformation.
The austenitic material 1.4567, which is comparable to both AISI 302 HQ and AISI 304 Cu, is a chromium-nickel stainless steel. It differs from the otherwise similar material 1.4301 / AISI 304 in its copper content of 3-4 %, which contributes to the fact that stainless steel 1.4567 is ideally suited for cold forming. It can also be used at low temperatures.The material 1.4567 has good forging properties and good corrosion resistance (but not to salt water). It is used, among other things, in the automotive industry and for the production of screws.
Customer Visit
GNEE Steel Group is China's professional one-stop supply chain enterprise for steel products. Its stainless steel pipe production technology has reached the world's average technical level. It has been recognized by dozens of project companies and has become a star enterprise in Asia.


Hot Tags: 1.4568 1.4567 stainless steel pipe reducer, China 1.4568 1.4567 stainless steel pipe reducer suppliers, Super Duplex Steel UNS S32750 Angle, 310 Butt Weld Flanges
You Might Also Like
Send Inquiry