Z275 Hot Dip Galvanized Steel Coils , Skin Pass , Astm A653 CSB Galvanized Steel Sheet
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of z275 hot dip galvanized steel coils , skin pass , astm a653 csb galvanized steel sheet in China. If you're going to wholesale high quality z275 hot dip galvanized steel coils , skin pass , astm a653 csb galvanized steel sheet made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Z275 Hot dip Galvanized Steel Coils , Skin Pass , Astm A653 CSB Galvanized Steel Sheet
Description
| Grade: | A653 CSB | Width: | 1000-2000mm |
|---|---|---|---|
| Length: | 2000-6000mm | Spangle: | Zero Spangle, Regular Spangle |
| Technique: | Cold Rolled | Surface Treatment: | Chromated And Oiled |
| High Light: |
hot dipped galvanized steel coils,galvanised steel coil |
||
galvanized steel coils are produced by immersing steel in a zinc bath. An appropriate galvanizing process requires a pretreatment process during which the steel passes through different baths which prepare the surface for zinc coating. In this stage, chemicals are used to clean the surface of the steel. After the chemical treatment, the steel coils pass through a bath of melted zinc at temperatures around 460 ° C. The resulting uniform coating is finished through a process of skin-passing to provide smooth and shiny appearance of the finished product. To store for a longer period, the hotdip galvanized coils can be delivered with a final oil coating, according to the customer's demand.
| product name | galvanized steel coils |
| thickness | 0.135mm-4.0mm |
| width | 600mm-1500mm762mm,914mm,1000mm,1200mm,1219mm,1250mm |
| zinc coating | 40g,60g, 80g, 90,100g, 120g, 140g,180g, 200g, 250g, 275g and so on. |
| standard | ASTM, AISI, DIN, GB |
| material |
SGCC,DC51D,DX51D,DX52D,,SGCD,Q195,Q235,SGHC,DX54D, S350 GD, S450 GD,S550 GD |
| spangle | zero spangle, regular spangle or normal spangle |
| surface treatment | chromated and oiled, chromated and non-oiled |
| packing | export standard. |
| payment | T/T, L/C or DP |
| min order | 25 tons (one 20ft FCL) |
| coil weight | 3-8ton or as client requirement. |
| quality | soft or hard quality |
| STEEL GRADE | CHEMICAL COMPOSITION % | MECHANIC PROPERTY | C.B OF COATING | COATING | |||||||||
| C | Si | Mn | S | P | T.S | Y.S | E.L | ||||||
| x103 | x103 | x102 | x103 | x103 | Mpa | Mpa | % | d=0 180° | G/M² | ||||
| JIS G3302 SGCC | 12 | 30 | 41 | 31 | 21 | 480 | 300 | 13 | OK | Z60-150 | |||
| JIS G3302 SGCH | 12 | 10 | 21 | 18 | 8 | 680 | 650 | OK | Z60-150 | ||||
| ASTM A653 CS.B | 20 | 30 | 60 | 35 | 30 | 386 | 205~380 | 20 | OK | Z80-275 | |||
| DX51D+Z | 29 | 21 | 18 | 1.8 | 11 | 355 | 245 | 38 | OK | Z80-275 | |||
| G550 | 20 | 6 | 73 | 5 | 17 | 715 | 654 | 8 | OK | Z80-275 |
|
||
Our advantage:
ISO System;
SGS and BV Audited company;
Management Systems-Internal Software;
Shipment of goods-more than 50 countries;
We have the most convenient transport and prompt delivery;
We offer competitive price with best service;
We have high technical production line with top quality products;
We have won high reputation based on best quality products;


Hot Tags: z275 hot dip galvanized steel coils , skin pass , astm a653 csb galvanized steel sheet, China z275 hot dip galvanized steel coils , skin pass , astm a653 csb galvanized steel sheet suppliers, AISI430 Stainless Steel Foil, 304 316 316l SS Cold Rolled Steel Coils, 316L Stainless Steel Coil, 2507 Stainless Steel Coil