Stainless Steel 436 Coil
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of stainless steel 436 coil in China. If you're going to wholesale high quality stainless steel 436 coil made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Stainless Steel 436 Coil
Product Introduction
The 436 stainless steel coil is a high-quality product with excellent performance in various industrial applications. With a thickness range of 0.3mm to 3mm and a width of 1000mm to 1500mm, this coil can be tailored to meet the requirements of any customer.
Introduction to matter
Name: Ferritic stainless steel
Standard: AISI, ASTM
Model: 436
UNS number: S43600
●Chemical composition of 436 steel①:
Carbon C: ≤0.12
Manganese Mn: ≤1.00
Silicon Si: ≤1.00
Chromium Cr: 16.0~18.0
Nickel Ni②:-
Phosphorus P: ≤0.04
Sulfur S: ≤0.03
Molybdenum Mo: 0.75~1.25
Niobium Nb: (5C~0.80)

Hot Tags: stainless steel 436 coil, China stainless steel 436 coil suppliers, AISI430 Stainless Steel Foil, 304 316 316l SS Cold Rolled Steel Coils, 316L Stainless Steel Coil, 2507 Stainless Steel Coil