Alloy 321 Stainless Steel Coil
video

Alloy 321 Stainless Steel Coil

Alloy 321 (UNS S32100) is a titanium stabilized austenitic stainless steel with good general corrosion resistance. It has excellent resistance to intergranular corrosion after exposure to temperatures in the chromium carbide precipitation range of 800 – 1500°F (427 – 816°C). The alloy resists oxidation to 1500°F (816°C) and has higher creep and stress rupture properties than alloys 304 and 304L. It also possesses good low temperature toughness.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of alloy 321 stainless steel coil in China. If you're going to wholesale high quality alloy 321 stainless steel coil made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Alloy 321 (UNS S32100) is a titanium stabilized austenitic stainless steel with good general corrosion resistance. It has excellent resistance to intergranular corrosion after exposure to temperatures in the chromium carbide precipitation range of 800 – 1500°F (427 – 816°C). The alloy resists oxidation to 1500°F (816°C) and has higher creep and stress rupture properties than alloys 304 and 304L. It also possesses good low temperature toughness.

4 98

Alloy 321H (UNS S 32109) is the higher carbon (0.04 – 0.10) version of the alloy. It was developed for enhanced creep resistance and for higher strength at temperatures above 1000oF (537°C). In most instances, the carbon content of the plate enables dual certification.

Denstiy
lbm/in3
Coefficient of
Thermal Expansion (min/in)-°F
Thermal Conductivity BTU/hr-ft-°F Specific Heat BTU/lbm -°F Modules of Elasticity (annealed)2-psi
at 68 °F at 68 – 212°F at 68 – 1832°F at 200°F at 32 – 212°F in tension (E)
0.286 9.2 20.5 9.3 0.12 28 x 106

4 154

Processing performance: 321 stainless steel has good processing properties and can be formed through conventional cold working and hot working processes. Cold working increases its strength and hardness, but intermediate annealing may be required to reduce stress.


Welding performance: 321 stainless steel has good welding properties and can be welded using most standard welding methods, including TIG (tungsten inert gas welding), MIG (metal inert gas welding) and resistance welding. No heat treatment is required after welding, and the stabilizing effect of titanium helps prevent intergranular corrosion during welding.

Hot Tags: alloy 321 stainless steel coil, China alloy 321 stainless steel coil suppliers, 2507 Stainless Steel Coil, AISI430 Stainless Steel Foil, 316L Stainless Steel Coil, 304 316 316l SS Cold Rolled Steel Coils

Send Inquiry

whatsapp

Phone

E-mail

Inquiry