Alloy 317/317L Stainless Steel Coil
video

Alloy 317/317L Stainless Steel Coil

Alloy 317L (UNS S31703) is a lowcarbon corrosion resistant austenitic chromium-nickel-molybdenum stainless steel. The high levels of these elements assure the alloy has superior chloride pitting and general corrosion resistance to the conventional 304/304L and 316/316L grades. The alloy provides improved resistance relative to 316L in strongly corrosive environments containing sulfurous media, chlorides, and other halides.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of alloy 317/317l stainless steel coil in China. If you're going to wholesale high quality alloy 317/317l stainless steel coil made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Alloy 317L (UNS S31703) is a lowcarbon corrosion resistant austenitic chromium-nickel-molybdenum stainless steel. The high levels of these elements assure the alloy has superior chloride pitting and general corrosion resistance to the conventional 304/304L and 316/316L grades. The alloy provides improved resistance relative to 316L in strongly corrosive environments containing sulfurous media, chlorides, and other halides.

 

The low carbon content of Alloy 317L enables it to be welded without intergranular corrosion resulting from chromium carbide precipitation enabling it to be used in the as-welded condition. With the addition of nitrogen as a strengthening agent, the alloy can be dual certified as Alloy 317 (UNS S31700).

4 136

Property Value
Density 0.285 lbs/in³ (7.89 g/cm³)
Specific Heat 0.12 BTU/lb-°F (32 – 212°F) / 502 J/kg-°K (0 – 100°C)
Modulus of Elasticity 29.0 x 10⁶ psi (200 GPa)
Thermal Conductivity 8.1 BTU/(hr x ft x °F) (14 W/(m x K)) at 68°F (20°C)
Melting Range 2540 – 2630°F (1390 – 1440°C)
Electrical Resistivity 33.5 Microhm-in at 68°F (85.1 Microhm-cm at 20°C)

Alloy 317L is non-magnetic in the annealed condition. It cannot be hardened by heat treatment, however the material will harden due to cold working. Alloy 317L can be easily welded and processed by standard shop fabrication practices.