AISI430 Stainless Steel Foil
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of aisi430 stainless steel foil in China. If you're going to wholesale high quality aisi430 stainless steel foil made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
430 stainless steel foil is a type of ferritic stainless steel that is commonly used for its excellent corrosion resistance and formability. It is known for its durability, making it suitable for various industrial and household applications.

| Category | Details |
|---|---|
| Chemical Composition | - Chromium (Cr): 16.0-18.0%<br>- Carbon (C): ≤ 0.12%<br>- Manganese (Mn): ≤ 1.00%<br>- Silicon (Si): ≤ 1.00%<br>- Phosphorus (P): ≤ 0.04%<br>- Sulfur (S): ≤ 0.03%<br>- Nickel (Ni): ≤ 0.75%<br>- Iron (Fe): Balance |
| Mechanical Properties | - Tensile Strength: 450-600 MPa<br>- Yield Strength: 205 MPa<br>- Elongation: 20%<br>- Hardness: 70-90 HRB |
| Physical Properties | - Density: 7.75 g/cm³<br>- Melting Point: 1425-1510°C<br>- Thermal Conductivity: 25 W/m·K (at 100°C)<br>- Electrical Resistivity: 600 nΩ·m (at 20°C) |