Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of 301ln 0.1 - 2.0mm s30153 aisi 301 1.4310 cold rolled stainless steel strip in China. If you're going to wholesale high quality 301ln 0.1 - 2.0mm s30153 aisi 301 1.4310 cold rolled stainless steel strip made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
301LN 0.1 - 2.0mm S30153 AISI 301 1.4310 Cold Rolled Stainless Steel Strip
Description
| Length: | Customer's Request,in Coil | Application: | Construction,Medical Instruments,Industry,Decoration |
|---|---|---|---|
| Type: | Cold Rolled Coil | Standard: | ASTM,AISI,JIS,DIN |
| Width: | 600--1800mm Al Available | Surface: | 2B,HL |
| Technique: | Cold Rolled | Thickness: | 0.1-2.0mm |
| Price Term: | CIF CFR FOB EX-WORK | ||
| High Light: |
s30153 cold rolled stainless steel strips,301ln cold rolled stainless steel strips,0.1mm stainless steel strip roll |
||
Cold Rolled 301LN Stainless Steel Strips 0.1 - 2.0mm SS Strips Stainless Steel Roll S30153
Specification of our stainless steel strip
| Products | 301LN Stainless Steel Strips |
| Thickness | 0.1 - 2.0mm |
| Width | 8 - 1219mm |
| Hardness | 1/4H 1/2H 3/4H FH |
| Original Manufacturer | TISCO POSCO |
| Other Grade | 201 301 304 316L 310S 321 410 420 430 .etc |
| MOQ | 300 Kgs |
| Deliver time | within 10 days |
Grade 301 is an austenitic stainless steel that has a high work-hardening rate. Grade 301LN stainless steel is similar to grade 301L but with low carbon for improved ductility and welding of heavy sections. Grade 301LN has higher nitrogen content so as to compensate for the lower carbon content.
The following datasheet provides an overview of grade 301LN stainless steel.
Chemical Composition of 301LN Stainless Steel
The chemical composition of grade 301LN stainless steel is outlined in the following table.
| Element | Content (%) |
|---|---|
| Iron, fe | Balance |
| Chromium, Cr | 16-18 |
| Nickel, Ni | 6-8 |
| Manganese, Mn | 2 max |
| Silicon, Si | 1 max |
| Nitrogen, N | 0.07-0.20 |
| Phosphorous, P | 0.045 max |
| Carbon, C | 0.03 max |
| Sulfur, S | 0.03 |
Mechanical Properties of 301LN Stainless Steel
The mechanical properties of grade 301LN stainless steel are displayed in the following table.
| Properties | Metric | Imperial |
|---|---|---|
| Tensile strength (Outokumpu typical, cold rolled strip/sheet; EN 10002-1) | 765 MPa | 111000 psi |
| Yield strength (@strain 0.200 %) | 350 MPa | 50800 psi |
| Elastic modulus | 193 GPa | 27992 ksi |
| Poisson's ratio | 0.300 | 0.300 |
| Elongation at break (in 50 mm) | 47% | 47% |
Equivalent materials to grade 301LN stainless steel are given below.
ASTM A666
JIS G4305
EN 10088-2
EN 1.4318
JIS SUS 301L
Applications of 301LN Stainless Steel
Grade 301LN stainless steel is primarily used in rail car structural components mostly roll-formed, brake-pressed or stretch-formed to profiles; however it can also be used flat.
The following are the other applications of grade 301LN steel:
Springs
Toaster
Curtain walls
Screen frames
Airframe sections
Stove element clips
Automotive wheel covers
Highway trailer components
Wiper blade holders and clips



Hot Tags: 301ln 0.1 - 2.0mm s30153 aisi 301 1.4310 cold rolled stainless steel strip, China 301ln 0.1 - 2.0mm s30153 aisi 301 1.4310 cold rolled stainless steel strip suppliers, 316L Stainless Steel Coil, AISI430 Stainless Steel Foil, 304 316 316l SS Cold Rolled Steel Coils, 2507 Stainless Steel Coil