Silicon Steel M36 Coil
video

Silicon Steel M36 Coil

Welcome to our product introduction of the M36 Silicon Steel Coil. As a manufacturer located in China, we take pride in offering high-quality products to our clients all over the world. The M36 Silicon Steel Coil is just one of the many products that we offer to our customers.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of silicon steel m36 coil in China. If you're going to wholesale high quality silicon steel m36 coil made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Silicon Steel M36 Coil

1. Introduction to silicon steel sheets
Silicon steel sheet is a special cold-rolled steel sheet used to manufacture electrical equipment such as motors and transformers. It has good magnetic permeability and low loss characteristics and is an efficient and energy-saving electrical material.
2. Chemical composition of silicon steel sheets
The chemical composition of silicon steel sheets is mainly composed of iron and silicon, and contains a certain proportion of carbon, manganese, sulfur, phosphorus and other elements. Among them, the silicon content of silicon steel sheets is between 3% and 4.5%, the carbon content is generally controlled between 0.02% and 0.04%, the manganese content is controlled between 0.5% and 1.0%, and the phosphorus and sulfur contents are low. Generally, Controlled between 0.01% and 0.03% respectively.
The high silicon content in silicon steel sheets is one of the key factors for the excellent magnetic properties of silicon steel sheets. Although the content of carbon, manganese, phosphorus, sulfur and other elements in silicon steel sheets is low, they have an important impact on the performance of silicon steel sheets and require precise control during the production process.
3. Production process of silicon steel sheets
The production process of silicon steel sheets mainly includes raw material selection, rolling and annealing. The production process of silicon steel sheets requires high precision, and the chemical composition, magnetic properties and mechanical properties of silicon steel sheets must be controlled. In terms of raw material selection and process control, different manufacturers will have different priorities and optimization directions, and the performance required by silicon steel sheets for different uses is not exactly the same.
 

5 25 700x500