Silicon Cold Rolled Grain Oriented Steel
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of silicon cold rolled grain oriented steel in China. If you're going to wholesale high quality silicon cold rolled grain oriented steel made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Silicon Cold Rolled Grain Oriented Steel
Product Description
Product Description
Silicon steel, also known as silicon steel Sheet or Electrical Steel, it is a ferro-silicon soft magnetic alloy steel with very low carbon content, usually containing 0.5% to 4.5% silicon. The addition of silicon can increase the resistivity and maximum permeability of iron to reduce the coercivity, iron loss and magnetic aging.
The difference between oriented silicon steel and non-oriented silicon steel
Non-oriented silicon steel: ferro-silicon alloy with very low carbon content. In the deformed and annealed steel sheet, its grains are distributed randomly. The silicon content of the alloy is 1.5% to 3.0%, or the sum of the silicon and aluminum content is 1.8% to 4.0%. The products are usually cold-rolled plates or strips, which are mainly used to manufacture motors and generators.
Product Parameters
| Type | Grade | Width | Max Core Loss @ P17/50 | Lamination Factor(%) | Induction @ B8 |
| Common Type | 23Q110 | 900-1200mm | 1.10w/kg | 97 | 1.85T |
| 27Q120 | 1.20w/kg | 97 | 1.85T | ||
| 30Q120 | 1.20w/kg | 98 | 1.84T | ||
| High Induction Type |
23QG085 | 900-1200mm | 0.85w/kg | 97 | 1.90T |
| 23QG090 | 0.90w/kg | 97 | 1.90T | ||
| 23QG095 | 0.95w/kg | 97 | 1.89T | ||
| 23QG100 | 1.00w/kg | 97 | 1.89T | ||
| 27QG095 | 0.95w/kg | 97 | 1.90T | ||
| 27QG100 | 1.00w/kg | 97 | 1.90T | ||
| 30QG100 | 1.00w/kg | 98 | 1.90T | ||
| 30QG105 | 1.05w/kg | 98 | 1.89T | ||
| Domain Refined High Induction Type(Laser) | 23R080 | 900-1200mm | 0.80w/kg | 97 | 1.89T |
| 23R085 | 0.85w/kg | 97 | 1.89T | ||
| 27R090 | 0.90w/kg | 97 | 1.89T | ||
| 27R095 | 0.95w/kg | 97 | 1.89T |
Hot Tags: silicon cold rolled grain oriented steel, China silicon cold rolled grain oriented steel suppliers, CRNGO Electrical Steel Coil