Silicon steel is a silicon iron alloy with a silicon content of 3%~ 5%.Divided into oriented silicon steel and non-oriented silicon steel, it is an important soft magnetic alloy which is indispensable for power, electron and military industry.Was once known as "the arts and crafts of steel products".
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of go electrical steel in China. If you're going to wholesale high quality go electrical steel made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Electrical steel usually referred to as cold-rolled electrical steel, can be divided into two major categories including grain-oriented electrical steel and non-oriented electrical steel. Grain-oriented electrical steel, with its easy magnetization direction parallel to the rolling direction, has excellent magnetic properties in this direction including low core loss, high permeability, and low magnetostriction, and is widely used in the transformer industry. Further, it can obtain lower core loss by domain refinement treatment. Meanwhile, non-oriented electrical steel, featured by a random distribution of grain orientation and magnetic isotropy, is widely applicable to the motor industry.

 

Insulating Coating

Insulating Coating

Coating types

M11

M21

Component

Chromium containing , semi organic coating

Chromium free, semi organic coating

Coating thickness(μm)

0.7~1.5

0.8~5.0

Interlayer resistance
(Ω•mm2 /slice)

≥100

≥100

Adhesive property

Class A or class B

Class A or class B

Punching property

Excellent

Excellent

Antirust property

Excellent

Excellent

Heat resisting property

Resistant annealing at 750 C, N2 protection, for 2h

Annealing resistance in general

CRO Silicon Steel

Oriented electrical steel

Features of GO electrical steel products

Excellent electromagnetic property

first-class equipment, leading manufacturing process and strict management ensure the excellent and stable electromagnetic property of GNEE GO electrical steel.

Outstanding processability

high accuracy dimension and excellent mechanical property are convenient for the users to slit, cut, and laminate.

Preeminent dimensional accuracy

GNEE leading equipment and manufacturing technology ensure good shape, smooth surface, uniform thickness, small intra-plate deviation, and high lamination factor.

Excellent surface coating property

GNEE electrical steel has a uniform surface coating with good adhesiveness, which can prevent the peeling of the coating during processing; the interlaminar insulation property is good.

More width options

the users can choose from sheet widths of 700-1200mm of GNEE GO electrical steel, so as to improve the utilization ratio of the material.

 

Fields of application

Fields of application

Grain-oriented electrical steel

Non-oriented electrical steel

Series G

Series P

Series R

Series A

Series AH

Series AR

Series AT

230~400

440~700

800~1300

230~470

600~1000

Rotators

Large-sized motors

√

 

 

√

 

 

 

 

 

 

Medium-sized motors

 

 

 

√

√

 

√

 

 

 

Compressor motors

 

 

 

√

√

√

√

√

√

 

General motors

 

 

 

√

√

√

√

√

√

 

Small-sized precision motors

 

 

 

√

√

√

√

 

√

√

Motors for electric cars

 

 

 

√

 

 

√

 

√

√

Static device

High-frequency motors

 

 

 

√

 

 

√

 

 

√

Large-sized transformers

√

√

√

 

 

 

 

 

 

 

Small-sized power transformers

√

√

√

√

√

√

√

√

√

 

Transformers for instruments

√

√

 

√

 

 

 

 

 

 

Reactors and magnetic amplifiers

√

√

√

√

 

 

 

 

 

 

Power switches

 

 

 

√

 

 

 

 

 

 

Transformers for welding

 

 

 

 

√

√

 

√

 

 

Voltage regulators

 

 

 

√

√

√

√

√

√

 

Magnetic sealers

√

√

 

√

√

 

 

 

 

 

Electromagnetic devices for accelerators

√

√

 

 

√

 

√

 

 

 

CRGO Electrical Silicon Steel Use

GOES Electrical Steel

Hot Tags: go electrical steel, China go electrical steel suppliers, CRNGO Electrical Steel Coil

Send Inquiry

whatsapp

Phone

E-mail

Inquiry