UMCo 50 Alloy Plate
video

UMCo 50 Alloy Plate

UMCo50 is a heat-resistant cobalt alloy that has excellent thermal shock resistance and wear resistance. It also shows great strength against sulfur-and vanadium-attacks. Another feature is its higher melting point compared to other cobalt base orl nickel base heat-resistant alloys. For example, the alloy used for skid rails at a steel mill undergoes regular use at 1,350°C. Thus UMCo50 shows successful results in the application related to heat treatments and furnaces where other alloys could not be used due to their low melting point.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of umco 50 alloy plate in China. If you're going to wholesale high quality umco 50 alloy plate made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

UMCo50 is a heat-resistant cobalt alloy that has excellent thermal shock resistance and wear resistance. It also shows great strength against sulfur-and vanadium-attacks. Another feature is its higher melting point compared to other cobalt base orl nickel base heat-resistant alloys. For example, the alloy used for skid rails at a steel mill undergoes regular use at 1,350°C. Thus UMCo50 shows successful results in the application related to heat treatments and furnaces where other alloys could not be used due to their low melting point.

 

 

Common Trade Names:

Cobalt 50 , UMCo 50, G-CoCr28 , W.Nr : 2.4778

Specifications:

BS ISO 11973

Shock Resistances:

Since thermal shock resistance was given first priority when developing UMCo-50, this alloy shows far more outstanding thermal shock resistance than the popularly used 25Cr-20Ni stainless steel. For example, even after repeating the heating and cooling cycle (1000-water cooling-7 seconds) for 500 times, no cracking occurred. As a practical example, the alloy was used for four and a half years as a tray which was heated up to 1000 in a heavy oil furnace to quench various quenching agents. Hardly any cracking occurred in UMCo-50, whereas the 25Cr-12Ni alloys were able to be used for only 8 months in average.

Wear Resistances:

As for the wear resistance of UMCo-50, hardly any deterioration was found after being used as a sintering bar for copper sulfide for 50 months. On the other hand, cast iron parts used till then were heavily corroded, oxidized and worn even though operations were conducted at 900, making them usable for only three and a half months.

Weldability:

UMCo-50 can be welded together by arc or oxy-acetylene methods. When higher wear resistance is required, weld additionally with BISHILITE (HARDFACING ALLOYS). When welding UMCo-50 to stainless steel or steel, MA-W welding rod can be used.

UMCo 50 Chemical Composition

% C Si Mn S P Ni Cr Co Mo Fe
Min 0.05 0.5 0.5 - - 2 27 48 1 Blance
Max 0.12 1 1 0.02 0.02 2.5 29 52 1.5 Blance

UMCo 50 Physical Properties

Specific gravity Melting temperature Electrical Resistivity (25°C) Thermal expansion (0∼1000°C) Specific thermal conductivity (22°C)
8.05 1380∼1395°C 82.5Ω•cm 16.8 X 10-6 /°C 0.022cal/cm/sec./°C

UMCo 50 Alloy Mechanical Properties

  Tensile strength kgf/mm2 Yield strength(0.2%)kgf/mm2 Elongation%
3mm Sheet (Flat rolled) 90∼118 37∼46 10∼28
3mm Sheet : 1100°C X 30'Annealed 80∼90 30∼37 10∼20

UMCo 50 Alloy High Temperature Hardness (Forgings)

Temperature (°C) Forgings (HV)
20 260
600 228
700 210
800 160
860 76
After work hardening 425

High Temperature Corrosion

  Temperature(°C) Time Reduced weight g/m2 Reduced weight g/m2/hr
Plate (Flat rolled) 1000 144hr 26∼83 0.18∼0.58
Plate (Flat rolled) 1200 144hr 200∼120 0.69∼0.83

UMCo 50 Available Shape

UMCo 50 Size Range

product-720-720product-720-720product-720-720product-720-720

 

FAQ

 

Q: How do you control quality ?
A: Mill Test Certification is supplied with shipment, Third Party Inspection is available. and we also get ISO,SGS,Alibaba Verified.
Q: What are the advantages of your company ?
A: We have many professionals, technical personnel, more competitive prices and best after-dales service than other stainless steel companies.
Q: How many coutries you already exported ?
A: Exported to more than 50 countries mainly from America, Russia, UK, Kuwait, Egypt, Turkey, Jordan,India, etc.
Q: Can you provide sample ?
A: Yes. We can provide the small samples in stock for free, as long as you contact us.Customized samples will take about 5-7 days.

 

Hot Tags: umco 50 alloy plate, China umco 50 alloy plate suppliers

Send Inquiry

whatsapp

Phone

E-mail

Inquiry