Inconel625/N06625(GH3625) solid solution strengthened alloy
Inconel625
1. Introduction to Inconel625:
Inconel625 is a Ni-Cr based solid solution strengthened deformed superalloy. It is a solid solution strengthened nickel based deformed superalloy with chromium, molybdenum and niobium as the main strengthening elements. It has a service temperature of 950°C and has good performance from low temperature to 980°C. It has good tensile properties and fatigue properties, processing and welding properties. The alloy has excellent corrosion resistance and oxidation resistance, and is resistant to stress corrosion in salt spray atmosphere. Therefore, Inconel625 can be widely used in manufacturing aerospace engine parts, aerospace structural components and chemical equipment. A variety of plates, bars, tubes, and forgings are available.


2. Inconel625 applications and features:
Inconel625 alloy has a very low corrosion rate in both marine and non-marine environments. It has good resistance to seawater corrosion, corrosion resistance to various salt solutions, good corrosion resistance to HNO3 and H3PO4, and good corrosion resistance to HCl and low-concentration H2SO4 heated below the boiling point. It also has considerable resistance. The alloy undergoes age hardening after long-term use at 550-700°C, which can lead to some decrease in the plasticity of the alloy. If you need to be resistant to high temperatures and corrosion, Shanghai Yuanding recommends using this material. It can be used in aviation equipment, as well as seawater pitting corrosion, chloride stress corrosion resistance, F-H3PO4 resistance, etc., such as the manufacture of thin-walled containers and pipe fittings, corrosion-resistant pipes, reactors, heat exchangers and valves, etc. GNEE will organize it for you. If you have any questions, please call us for consultation.