Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of nickel inconel alloy 602ca in China. If you're going to wholesale high quality nickel inconel alloy 602ca made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Nickel Inconel Alloy 602CA
Inconel 602CA is one of the most oxidation resistant nickel alloy available. Outstanding oxidation resistance is achieved through a high chromium content (25%) supplemented with aluminum (2.2%) and a microalloying addition of yttrium (0.1%). High chromium contents are known to be beneficial for resisting oxidation. The aluminum addition allows for the formation of a continuous homogenous self repairing AI2O3 subscale. The addition of yttrium improves the adhesion and spalling resistance of the chromium and aluminum oxide scales.
Nickel Alloy 602CA Chemical Composition
| % | Ni | Cr | Cu | C | Mn | Si | Y | Fe | Ti | Al | Zr |
|---|---|---|---|---|---|---|---|---|---|---|---|
| Min | Balance | 24 | 0 | 0.15 | 0 | 0 | 0.05 | 8 | 0.1 | 1.8 | 0.01 |
| Max | Balance | 26 | 0.1 | 0.25 | 0.15 | 0.5 | 0.12 | 11 | 0.2 | 2.4 | 0.1 |
Inconel Alloy 602CA Physical Properties
| Density g/cm3 | Melting range | Specific heat capacity J/kg | Thermal conductivity W/m | Electrical resistivity |
|---|---|---|---|---|
| 7.9 | 1340-1400 | 450 | 11.3 | 1.15 |

Key Properties and Characteristics Of Inconel 602CA:
High-temperature strength: Inconel 602CA exhibits excellent strength and mechanical properties at elevated temperatures, making it suitable for applications in extreme heat environments.
Oxidation resistance: The high chromium content in Inconel 602CA provides exceptional resistance to oxidation, enabling it to withstand high-temperature oxidizing atmospheres.
Carburization and sulfidation resistance: This alloy demonstrates good resistance to carburization and sulfidation, which are processes involving the diffusion of carbon and sulfur into the material at high temperatures. This resistance is beneficial for applications in petrochemical, chemical, and power generation industries.
Creep resistance: Inconel 602CA has good resistance to creep deformation, which is important for applications subjected to prolonged exposure to high temperatures and constant stress.
Weldability: Inconel 602CA can be readily welded using common welding techniques, allowing for the fabrication and repair of components.