Inconel X750 Sheet
Shape: Round
Temper:
.75 IN Round X-750 NICKEL CG, EQUALIZED, 120.0000-168.0000 IN Length
Specs: ASTM.B637,DIN.EN10204,AMS.5667,PWA.300,GE.S400,UNS.N07750,PWA.MCL-F17,GE.S1000
LBS/FT: 1.58
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of inconel x750 sheet in China. If you're going to wholesale high quality inconel x750 sheet made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Inconel X-750 is one of numerous metal alloys sold by American Elements under the trade name AE Alloys. Generally immediately available in most volumes, AE Alloys are available as bar, ingot, ribbon, wire, shot, sheet, and foil. Ultra high purity and high purity forms also include metal powder, submicron powder and nanoscale, targets for thin film deposition, and pellets for chemical vapor deposition (CVD) and physical vapor deposition (PVD) applications. American Elements produces to many standard grades when applicable, including Mil Spec (military grade); ACS, Reagent and Technical Grade; Food, Agricultural and Pharmaceutical Grade; Optical Grade, USP and EP/BP (European Pharmacopoeia/British Pharmacopoeia) and follows applicable ASTM testing standards. Typical and custom packaging is available. Primary applications include bearing assembly, ballast, casting, step soldering, and radiation shielding.
Product Parameter
|
Element |
Min % |
Max % |
|
C |
– |
0.08 |
|
Mn |
– |
1.00 |
|
Si |
– |
0.50 |
|
S |
– |
0.01 |
|
Cr |
14.00 |
17.00 |
|
Ni |
70.00 |
– |
|
Nb/Cb |
0.70 |
1.20 |
|
Ti |
2.25 |
2.75 |
|
Al |
0.40 |
1.00 |
|
Fe |
5.00 |
9.00 |
|
Co |
– |
1.00 |
|
Ta |
– |
0.05 |
|
Cu |
– |
0.50 |
Feature
Alloy X-750 is austenitic under all conditions. The alloy is heat treated by several different methods depending upon the application or requirement. Two common treatments are:
1. For maximum creep, relaxtion and rupture strength at temperatures above 1100°F (593°C):
Solution Treatment - 1800°F (982°C), time commensurate with thickness, air cool.
Intermediate Age - 1550°F (843°C), 24 hrs, air cool.
Final Age -1300°F (704°C), 20 hrs, air cool.
2. For highest room temperature yield strength and tensile ductility:
Stress Equaliztation - 1625°F (885°C), 24 hrs, air cool.
Precipitation Age - 1300°F (704°C), 20 hrs, air cool.
Application
The alloy has good corrosion resistance and creep rupture strength in high temperature environments, good mechanical properties, and is widely used. It has sufficient strength and corrosion resistance and oxidation resistance below 980.
1. Manufacture springs and bolts that work at high temperatures; rotor blades, impellers and other structural parts on gas turbines;
2. The thrust chamber on the rocket engine;
3. Thrust reverse device on the aircraft;
4. Large high-pressure vessel.
Our Company

38000㎡ workshop and 200+ emplovees to meet your huge demands.
Packing & Delivery

Our nickel based bars are packaged professionally to ensure they remain intact during transportation and storage. Our packaging materials have been carefully selected to protect nickel based bars from moisture, pollution, and damage. We can provide different packaging methods according to your requirements, such as wooden boxes, pallets, cardboard boxes, etc., to meet your specific needs. Our packaging process strictly follows international standards to ensure that the nickel based bars you receive are high-quality and undamaged products. No matter how much quantity or size you need, we can provide you with efficient, reliable, and satisfactory services. Please contact us for more information.
Customer Visit

Gnee exports steel to over 70 countries and collaborates with more than 600 companies worldwide
FAQ
Q: How many coutries you already exported ?
A: Exported to more than 50 countries mainly from America, UK, Kuwait, Egypt, Turkey, Jordan,India, etc.
Q: Can you provide sample ?
A: Yes. We can provide the small samples in stock for free, as long as you contact us.Customized samples will take about 5-7 days.
Q:Can you send samples?
A:Of course, we can send samples to all parts of the world, our samples are free, but customers need to bear the courier costs.
Q:What product information do I need to provide?
A:You need to provide the grade, width, thickness, coating and the number of tons you need to purchase.