Inconel Alloy 601GC Seamless high precision Pipe
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of inconel alloy 601gc seamless high precision pipe in China. If you're going to wholesale high quality inconel alloy 601gc seamless high precision pipe made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Inconel 601GC Seamless high precision Pipe introduce
Alloy 601GC Seamless high precision Pipe


Super alloys or high performance alloys have good creep and oxidation resistance. They have the capacity to function in environments with high temperatures and mechanical stress, and also where high surface stability is required. They are divided into three types, which are cobalt-based, nickel-based, and iron-based alloys. They can be used at temperatures above 540°C (1000°F).
Inconel 601G is a grain controlled version of Inconel 601. Nitrogen and zirconium are added to control the grain growth. The following datasheet gives an overview of Inconel 601GC.
As a leading supplier and manufacturer in China, Gnee Steel offers cost-effective Inconel 601GC products.
INCONEL 601GC alloy is a nickel-chromium-iron alloy with additions of aluminum, zirconium, and nitrogen. High levels of nickel and chromium give the alloy excellent high-temperature strength and corrosion resistance. The aluminum content further enhances its oxidation resistance.
INCONEL 601GC alloy is a grain-controlled version of INCONEL 601 alloy (UNS N06601). Zirconium and nitrogen in INCONEL 601GC alloy inhibit grain growth at high temperatures. Grain size stability is an important factor in achieving optimal high-temperature performance and service life.
The properties of INCONEL 601GC alloy are particularly suitable for seam-welded roller tubes in roller-hearth furnaces that produce glazed ceramic tiles. The alloy has sufficient strength and resistance to oxidation and corrosion to meet the long-term, economical operation of these continuous-firing ceramic tile kilns.
Chemical Composition
The following table shows the chemical composition of Inconel 601GC.
| Elements | Contents (%) |
|---|---|
| Nickel, Ni | 58-63 |
| Chromium, Cr | 21-25 |
| Iron, Fe | 15 |
| Copper, Cu | 1.0 |
| Manganese, Mn | 1.0 |
| Carbon, C | 1.0 |
| Silicon, Si | 1.0 |
| Aluminum, Al | 0.80-1.70 |
| Nitrogen, N | 0.020-0.070 |
| Zirconium, Zr | 0.070-0.25 |
| Sulfur, S | 0.015 |
Physical Properties
The physical properties of Inconel 601GC are given in the following table.
| Properties | Metric | Imperial |
|---|---|---|
| Density | 8.11 g/cm³ | 0.293 lb/in³ |
| Melting point | 1301-1368°C | 2374-2494°F |
Inconel Alloy 601GC ss high precision Pipe



GNEE Group Factory Environment
Inconel Alloy 601GC precision Pipe

GNEE Group Product Packaging
Inconel Alloy 601GC high precision Pipe

FAQ
Q: How many coutries you already exported ?
A: Exported to more than 50 countries mainly from America, UK, Kuwait, Egypt, Turkey, Jordan,India, etc.
Q: Can you provide sample ?
A: Yes. We can provide the small samples in stock for free, as long as you contact us.Customized samples will take about 5-7 days.
Q: Will the Test Certificate meet EN10204 3.1/3.2?
A: We will provide Original Mill Test Certificate certified to EN10204 3.1/3.2 for products in stock or further processing needed.
Q: How long is your delivery time?
A: Generally it is 2-5 days if the goods are in stock or it will need 7-20 days if the goods need to be customized.
Hot Tags: Inconel Alloy 601GC Seamless high precision Pipe, China Inconel Alloy 601GC Seamless high precision Pipe suppliers, inconel alloy resonator parts, inconel piping, inconel alloy detector parts, Inconel 718 Alloy Plate, inconel alloy diode parts, inconel alloy amplifier parts
You Might Also Like
Send Inquiry