Inconel 751
video

Inconel 751

INCONEL® alloy 751 (UNS N07751) is a precipitation hardenable nickel-chromium alloy, used mainly for the exhaust valves of internal combustion engines. Its thermal properties correspond closely to those published for INCONEL alloy X-750.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of inconel 751 in China. If you're going to wholesale high quality inconel 751 made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Overview

As a leading supplier & manufacturer in China, AEETHER supply cost-effective Inconel 751 Products.

INCONEL® alloy 751 (UNS N07751) is a precipitation hardenable nickel-chromium alloy, used mainly for the exhaust valves of internal combustion engines. Its thermal properties correspond closely to those published for INCONEL alloy X-750.

In the evaluation of materials for exhaust valve applications, nickel-chromium alloys have performed well in a 1675°F (913°C) lead oxide screening test. INCONEL alloy 751 repeatedly offered good results, with corrosion rates averaging 4.31 g/dm2/h. Like other nickel-chromium alloys, INCONEL alloy 751 also resists attack by other exhaust stream impurities such as sulfur, bromine and chlorine.

The hot working range for INCONEL alloy 751 is 1800- 2200°F (980-1205°C). The alloy should be reheated to 2200°F (1205°C) whenever its temperature falls below 1800°F (980°C).

INCONEL alloy 751 is readily machined in the as-hot finished condition. The best procedure is to machine to slightly oversize, precipitation heat treat, then finish to size. A slight permanent contraction (about 0.0003 in/in) takes place during precipitation. Precipitation treated material can be finish machined to fine finishes and close tolerances, and will have good dimensional stability.

 

product-720-720product-720-720product-720-720product-720-720

 

Chemical Composition

Data Sheet

Physical Properties

Density g/cm3 8.22
lb/in.3 0.297
Melting Range °F 2540 - 2600
°C 1390 - 1430
Specific Heat Btu/lb-°F 0.103
J/kg-°C 431
Electrical Resistivity ohm-circ mil/ft 731
μΩ-m 1.22
Curie Temperature °F -193
°C -125
Permeability at 200 oersted 15.9 kA/m 1.0035

Mechanical Properties

Temperature Tensile Strength Yield Strength
(0.2% Offset)
Elongation Reduction of Area Hardness
°F °C ksi MPa ksi MPa % % BHN
Room Room 141.5 976 190.0 1310 22.5 38.2 352
1200 649 128.9 889 159.6 1100 22.5 32.1 291
1350 732 113.5 783 124.8 860 18.5 25.7 235
1500 816 76.3 526 80.3 554 26.0 35.9 173

FAQ

 

Q: How do you control quality ?
A: Mill Test Certification is supplied with shipment, Third Party Inspection is available. and we also get ISO,SGS,Alibaba Verified.
Q: What are the advantages of your company ?
A: We have many professionals, technical personnel, more competitive prices and best after-dales service than other stainless steel companies.
Q: How many coutries you already exported ?
A: Exported to more than 50 countries mainly from America, UK, Kuwait, Egypt, Turkey, Jordan,India, etc.
Q: Can you provide sample ?
A: Yes. We can provide the small samples in stock for free, as long as you contact us.Customized samples will take about 5-7 days.

Hot Tags: inconel 751, China inconel 751 suppliers, inconel alloy compressor parts, Inconel UNS N07718 Pipe Fitting, inconel alloy elbow fittings, inconel alloy electrical system parts, inconel alloy valve parts, inconel alloy metal tube

Send Inquiry

whatsapp

Phone

E-mail

Inquiry