Inconel 740H
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of inconel 740h in China. If you're going to wholesale high quality inconel 740h made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Overview
As a leading supplier & manufacturer in China, AEETHER supply cost-effective Inconel 740H Products.
As the world's demand for electrical power increases, governments also demand that emissions be strictly controlled to minimize the greenhouse effects of society's carbon footprint. Despite that situation, coal, oil and gas continue to be the major fuels for power generation facilities. While nuclear, gas turbine, solar and wind generation are expected to increase, coal is still predicted to fuel 37% of the world's electrical generating capacity in 2035.1 Thus, there is a strong impetus for development of cleaner, more efficient power generation. The efficiency of fossil fuel-fired boilers increases with operating temperature and pressure. There have been progressive increases in these conditions for boiler design culminating in advanced ultra-supercritical (A-USC) technology. A-USC boilers are expected to offer levels of generation efficiency over 50%(HHV) and their operation is such that carbon-base emissions can be readily collected and sequestered.
Programs to develop A-USC capability are currently active around the world. Since A-USC plants will operate at higher temperatures (700° to 760°C) and pressures (up to 35 MPa), nickel-base superalloys are required to meet the rigors of strength and corrosion resistance. INCONEL® alloy 740H® was developed specifically to operate under these demanding service conditions.
INCONEL alloy 740H is a nickel-base, precipitation hardenable superalloy that offers a unique combination of high strength and creep resistance at elevated temperatures along with resistance to coal ash corrosion. The alloy was originally targeted for use as A-USC boiler tubes in the superheater sections of these plants but was then adapted for application as a material for the steam headers to which the boiler tubes are connected. A-USC boiler tubes are conventional sizes [typically 1.5 to 3 inch (38 to 76 mm) outside diameter]. Main steam header pipe sizes occupy a much larger size range, with outer diameter greater than 12 inches (305 mm) and wall thickness likely exceeding 1.5 inches (38 mm). Seamless steam reheat piping, at up to 30 inch (760 mm) outer diameter, is also a feasible product line with INCONEL alloy 740H.
Corrosion Resistance
With its high content of chromium, alloy 740H offers excellent resistance to corrosion at elevated temperatures. This is especially important for boiler tubes as they are exposed to fireside corrosion on the exterior and steamside corrosion on the interior. Alloy 740H has been extensively evaluated under both sets of conditions.
More +
Main Standards
ASTM B983
Seamless Pipe & Tube
AWS A5.14 ERNiCrMo-15
Filler Metal
Chemical Composition
Data Sheet
Physical Properties
| Density | g/cm3 | 8.05 | |
|---|---|---|---|
| lb/in.3 | 0.291 | ||
| Melting Range | °F | 2350 - 2484 | |
| °C | 1288 - 1362 | ||
| Electrical Resistivity | Ω-circ mil/ft | 702.7 | |
| μ Ω -m | 1.168 | ||
Mechanical Properties
| Test Temperature °F (°C) |
0.2% Yield Strength, Ksi (MPa) |
Ultimate Tensile Strength, Ksi (MPa) |
Elongation % | Reduction of Area % |
|---|---|---|---|---|
| Transverse Orientation | ||||
| Room Temp. | 105 (724) | 154.6 (1066) | 23.7 | 28.1 |
| 1292°F (700°C) | 82.2 (567) | 124.9 (861) | 17 | 23.1 |
| 1337°F (725°C) | 85.4 (589) | 125 (862) | 22.8 | 37.4 |
| 1382°F (750°C) | 86.4 (596) | 118.6 (818) | 23.9 | 28.7 |
| 1424°F (775°C) | 80.8 (557) | 110.1 (759) | 22.1 | 30.7 |
| 1472°F (800°C) | 86.2 (594) | 100.2 (691) | 23.5 | 31.2 |
| Longitudinal Orientation | ||||
| Room Temp. | 107.7 (742) | 164.4 (1133) | 24.3 | 39.8 |
| 1292°F (700°C) | 88.2 (608) | 132.3 (912) | 31.9 | 35.7 |
| 1337°F (725°C) | 87 (560) | 126.3 (871) | 28.4 | 34.4 |
| 1382°F (750°C) | 83.5 (576) | 118.2 (815) | 22.9 | 24 |
| 1424°F (775°C) | 81.8 (564) | 111.1 (766) | 27.9 | 37.1 |
| 1472°F (800°C) | 79.3 (547) | 100 (689) | 31.5 | 40.9 |




FAQ
Q: How do you control quality ?
A: Mill Test Certification is supplied with shipment, Third Party Inspection is available. and we also get ISO,SGS,Alibaba Verified.
Q: What are the advantages of your company ?
A: We have many professionals, technical personnel, more competitive prices and best after-dales service than other stainless steel companies.
Q: How many coutries you already exported ?
A: Exported to more than 50 countries mainly from America, Russia, UK, Kuwait, Egypt, Turkey, Jordan,India, etc.
Q: Can you provide sample ?
A: Yes. We can provide the small samples in stock for free, as long as you contact us.Customized samples will take about 5-7 days.
Hot Tags: inconel 740h, China inconel 740h suppliers, lnconelx 750 bar, inconel alloy inductor parts, inconel alloy seamless piping, inconel alloy flange fittings, inconel alloy spinning process, inconel alloy actuator parts
Previous
Inconel X-750 Alloy TubeNext
Inconel 725You Might Also Like
Send Inquiry