Heat Resistant Inconel 617 Uns N06617 Nickel Alloy Plate Sheet
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of heat resistant inconel 617 uns n06617 nickel alloy plate sheet in China. If you're going to wholesale high quality heat resistant inconel 617 uns n06617 nickel alloy plate sheet made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Heat Resistant Inconel 617 Uns N06617 Nickel Alloy Plate Sheet
Product Description
1.Product Name: Nickel Alloy Plate/Sheet
2.Grade: INCONEL 617 (UNS N06617/W. NR. 2.4663A)
3.Thickness: 0.6mm-70mm, Length:≤12000mm, Wide:≤2500mm
4.Features: Alloy 617 has excellent resistance to oxidation and carburization at high temperatures. It also resists a wide range of corrosive aqueous environments. Alloy 617 has high strength and maintains much of its strength at elevated temperatures.
5.Applications: Gas turbine engine combustion cans and ducts, heat treating equipment, petrochemical processing, power plant equipment, and catalyst-grid supports in nitric acid production.
6.Physical Properties
| Density | Melting Range | Elastic Die | Thermal Conductivity |
| g/cm3 | °C | N/mm2 | % |
| 8.4 | 1320-1370 | 212 | 13.4 |
7.The Minimum Mechanical Properties At Normal Temperature
| Alloy and State | Tensile Strength | Yield Strength | Rate of Elongation |
| Rm N/mm2 | RP0.2N/mm2 | A5% | |
| Solution Treatment | 680 | 300 | 30 |
8.Chemical Composition
| % | Ni | Cr | C | Mn | Si | P | S | Mo | Cu | Ti | Al | Co |
| MIN | - | 20 | 0.05 | - | - | - | - | 8 | - | - | 0.8 | 10 |
| MAX | 44.5 | 24 | 0.15 | 1 | 1 | 0.012 | 0.015 | 10 | 0.5 | 0.6 | 1.5 | 13 |


Hot Tags: heat resistant inconel 617 uns n06617 nickel alloy plate sheet, China heat resistant inconel 617 uns n06617 nickel alloy plate sheet suppliers, Inconel 617 Super Stainless Pipe, Inconel alloy material, inconel alloy camshaft parts, nickel-based, Inconel 825 Astm Standard, inconel alloy heating system parts