ASTM B444 Inconel 625 Capillary Tube
video

ASTM B444 Inconel 625 Capillary Tube

Standard: ASTM B444 (ASME SB444)
Alloy Grade: Inconel 625
UNS No: N06625
Material No.(W.Nr): 2.4856
Product Form: Seamless cold‑drawn capillary / micro tube
Dimension Range: OD 0.20‑10.00 mm;Wall 0.05‑2.00 mm;Max length 6000 mm
Dimensional Tolerance: ±0.005 mm ~ ±0.05 mm
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of astm b444 inconel 625 capillary tube in China. If you're going to wholesale high quality astm b444 inconel 625 capillary tube made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

ASTM B444 Inconel 625 capillary tube is a precision seamless nickel alloy tube (UNS N06625) engineered for heat exchanger service. Reinforced by molybdenum and niobium, it delivers stable strength from cryogenic conditions up to 980°C. It resists chloride pitting, crevice attack and stress corrosion cracking, maintaining integrity in aggressive process media. Fine dimensional tolerance supports consistent heat transfer efficiency. It retains high ductility after bending, meets strict NDT and traceability requirements, and serves long-cycle corrosive heat exchange systems in chemical, offshore and energy projects.

 

 

ASTM B444 Inconel 625 Capillary Tube

 

What is Inconel 625 Nickel Alloy?

Inconel 625 (UNS N06625) is a solid-solution strengthened nickel-based alloy reinforced by a combination of molybdenum and niobium, requiring no precipitation hardening heat treatment. It offers exceptional resistance to pitting and crevice corrosion as well as a wide range of complex corrosive media, making it a premier general-purpose grade for the chemical, marine, and oil & gas industries.

product-465-333

Our High-Performance, Corrosion-Resistant Inconel 625 Alloy Capillary Tubes are engineered to excel in the most demanding environments. Whether you're in chemical processing, aerospace, marine engineering, or pollution control, these tubes provide the reliability, durability, and performance you need to succeed. With exceptional corrosion resistance, high strength, and versatility, Inconel 625 is the material of choice for applications where failure is not an option. 

 

Inconel 625 Capillary Tube chemical composition

 

product-1057-183

 

Inconel 625 Capillary Tube Mechanical Properties

 

The below mechanical properties of Inconel 625 capillary tube conform to ASTM B444, tested at room temperature. These steady tensile strength and ductility values guarantee reliable bending, forming and long-term operation for heat exchanger precision tubing under corrosive conditions.

 

Property Requirement
Tensile Strength, min 690 MPa (100 ksi)
Yield Strength (0.2% offset), min 276 MPa (40 ksi)
Elongation in 50 mm, min 30 %
Hardness, max 95 HRB

 

Inconel 625 Micro-Tubing Size Specifications Table

 

Item Specification
Outside Diameter (OD) 0.20 mm - 10.00 mm
Inside Diameter (ID) 0.05 mm - 6.00 mm
Wall Thickness (WT) 0.05 mm - 2.00 mm
Length Up to 6000 mm
Tolerance ±0.005 mm to ± 0.05 mm
Surface Finish Bright Annealed (BA), Pickled, Polished

 

 Popular Incoloy 825 Micro Tube Sizes:

OD × WT (mm)
0.20 × 0.05
0.30 × 0.05
0.50 × 0.10
0.71 × 0.10
1.00 × 0.15
1.50 × 0.20
2.00 × 0.20
3.00 × 0.30
4.00 × 0.50
6.00 × 0.50

Custom sizes available according to customer drawings.

 

Inconel 625 Heat Treatment Classification (GR.1 & GR.2, ASTM B444)

 

Grade 1 (Solution Annealed)

Heating temperature: 1095–1205 ℃, air cool or water quench. Grain size ASTM 5–9. Delivers minimum tensile strength 690 MPa, minimum yield strength 276 MPa. Suitable for bending, coiling and further forming of capillary tubes.

 

Grade 2 (Stress Relieved)

Heating temperature: 870–980 ℃, slow cooling. No major grain growth. Residual stress reduced by 75% or higher. Tensile and yield strength stay close to GR1, applied for finished capillary tubes after shaping.

 

Advantages of Inconel 625 Capillary Tube

 

  • Service temperature range: -269 ℃ to 980 ℃, maintains stable mechanical performance across cryogenic and high-temperature conditions
  • Pitting resistance equivalent number (PREN) ≥ 48, resists chloride pitting and crevice corrosion in sour, seawater environments
  • Minimum elongation 30% (annealed state), supports tight-radius bending without cracking for heat exchanger coil fabrication
  • Molybdenum and niobium alloying elements suppress intermetallic precipitation below 650 ℃
  • Complies with ASTM B444, supports 100% eddy current test and material traceability for energy and nuclear instrument piping

 

Typical Applications of Inconel 625 Capillary Tube

 

Hydrogen Energy Systems

  • Hydrogen Pre-Cooling Systems
  • Hydrogen Refueling Stations
  • Hydrogen Compressors
  • Fuel Cell Cooling Systems

LNG & Cryogenic Equipment

  • LNG Vaporizers
  • LNG Heat Exchangers
  • Liquid Hydrogen Transfer Systems
  • Cryogenic Process Equipment

Oil & Gas Industry

  • Sour Gas Wells
  • Offshore Platforms
  • Subsea Equipment
  • Chemical Injection Lines

Chemical Processing Industry

  • Acid Transfer Systems
  • Chemical Reactors
  • Corrosion Resistant Tubing Systems

Heat Exchanger Industry

  • Shell & Tube Heat Exchangers
  • Compact Heat Exchangers
  • Microtube Heat Exchangers

Marine & Offshore Industry

  • Seawater Cooling Systems
  • Offshore Production Facilities
  • Marine Heat Transfer Equipment

Nuclear Power Industry

  • Auxiliary Heat Transfer Systems
  • Corrosion Resistant Tubing Assemblies

Instrumentation & Process Control

  • Precision Fluid Systems
  • Sampling Systems
  • Process Instrumentation

 

Why choose GNEE as your supplier for Inconel 625 capillary tubes?

 

Strictly manufactured to ASTM B444, supporting both GR1 solution annealed and GR2 stress-relieved heat treatment states as specified. 

 

product-877-240

Full inspection workflow: 100% eddy current testing, PMI verification, and mechanical property sampling. EN 10204 3.1 MTC is supplied with each batch for complete heat traceability.

 

Custom precision processing available, including cutting, coiling and U-bending for heat exchanger assemblies. Small-batch prototype orders and bulk project orders are both acceptable.

 

product-766-287

 

Dedicated anti-scratch, moisture-proof packaging for thin-wall capillary to avoid deformation and surface damage during ocean transit.

 

On-site technical support for material selection, forming guidance and corrosion matching, covering hydrogen energy, cryogenic, nuclear and offshore heat exchanger projects.

 

Submit your drawing and technical requirements, we will provide certified ASTM B444 Inconel 625 capillary tube solutions and quotation within 24 hours.

 

Contact us for the latest export price quote for Inconel 625 Capillary Tube

 

 

Hot Tags: astm b444 inconel 625 capillary tube, China astm b444 inconel 625 capillary tube suppliers, 625LCF 693 Stainless Steel Pipe, 625LCF Inconel ss Steel Pipe, Inconel 600 Plate, inconel alloy combustion chamber parts, inconel alloy connecting rod parts, UNS N06625 elbow

Send Inquiry

whatsapp

Phone

E-mail

Inquiry