Inconel 713 high temperature alloy has excellent chemical composition and physical properties, including the content of the main elements nickel,
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction
Inconel Pipe Products Description

713 693 inconel seamless tubing video

Chemical Composition Range of Alloy 713:

Nickel (Ni): 57.0% - 63.0%

Chromium (Cr): 9.0% - 12.0%

Iron (Fe): Balancing element

Aluminum (Al): 5.5% - 6.7%

Cobalt (Co): 5.0% - 6.5%

Titanium (Ti): 2.7% - 3.3%

Molybdenum (Mo): 2.5% - 3.0%

Carbon (C): 0.15% - 0.20%

Inconel Material Specification

 

Cr Mo Al Ti Nb Ni C
11.5-13.5% 3.8-4.8% 5.5-6.4% 0.5-1.0% 1.8-2.5% Balance 0.08-0.16%
Fe O          
≤1.0% ≤0.01%          

713 693 inconel pipe seamless

713 inconel pipe ss suppliers693 inconel pipe seamless steel dealer

 

Inconel 713 high temperature alloy has excellent chemical composition and physical properties, including the content of the main elements nickel, chromium, iron, aluminum and titanium, as well as advantages in high temperature strength, corrosion resistance, oxidation resistance and processing performance, and is suitable for high temperature applications and applications in extreme environments.
Inconel 693/UNS N06693 nickel-based superalloy is mainly composed of nickel (Ni) and iron (Fe), with the nickel content being approximately 50% to 60%. In addition, Inconel 693 also contains elements such as chromium (Cr), molybdenum (Mo), aluminum (Al), titanium (Ti), niobium (Nb), and may contain small amounts of carbon (C), copper (Cu), manganese ( Mn) and other impurity elements.

Customer Case

customer visit

713 693 inconel pipe price

713 693 inconel tubing factory

FAQ

Q: Are you a factory or a trading company?
A: We are a professional manufacturer, and our company is also a very professional steel products trading company. We can offer a wide range of steel as well as super stainless steel products.

Q: What does your factory do in terms of quality control?
A: We have obtained ISO, CE and other certifications. From materials to products, we check every process to maintain good quality.

Q: Can I get a sample before ordering?
Answer: Yes, of course. Usually our samples are free. We can produce according to your samples or technical drawings.

Q: About the product price of 713 693 inconel pipe seamless?
A: Due to cyclical changes in raw material prices, prices vary in different periods.

Contact Us

 

Address

No.4-1114 Beichen Building, Beicang Town, Beicheng District, Tianjin City, China

 

Phone

+86-15824687445

 

Email

ss@gneesteel.com

 

Skype

mmkelly1314

 

Whatsapp/Wechat

+86 15824687445

 

Hot Tags: 713 693 inconel pipe seamless, China 713 693 inconel pipe seamless suppliers, high nickel corrosion alloys, alloy pipe, alloy inconel piping, alloy seamless tubing, Inconel alloy material, alloy tubing

Send Inquiry

whatsapp

Phone

E-mail

Inquiry