690 718 Inconel Alloy Pipe
GNEE Group offers Nickel Alloy Inconel 690 718 in a variety of forms, including:
Bars
Wires
Sheets
Forgings
Tubes
Flanges
Seamless and Welded Pipes
Welding Rods
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of 690 718 inconel alloy pipe in China. If you're going to wholesale high quality 690 718 inconel alloy pipe made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
690 718 Inconel Alloy Pipe Application & Equivalent grade
690 718 Inconel Alloy Pipe video
GNEE STEEL GROUP supplies 690 718 Inconel Alloy Pipe for you
GNEE STEEL GROUP Inconel 690:
| STANDARD | UNS | WERKSTOFF NR. |
| Inconel Alloy 690 | N06690 | 2.4642 |
| GNEE STEEL GROUP Inconel 690 FORM | SIZE RANGE FROM | SIZE RANGE TO |
| Alloy 690 pipe | 0.5 in | 8 in |
| Alloy 690 tube | 12 mm | 260 mm |
| Alloy 690 pipe fittings | 0.5 in | 8 in |
| Alloy 690 flanges | 0.5 in | 8 in |
GNEE STEEL GROUP supplies Inconel 718
UNS: N07718
W. NR.: 2.4668
ASTM: B 637, B 670
ASME: CASE 2222-1, SFA 5.14
AMS: 5596, 5662, 5663, 5832
GE: B50TF14, B50TF15
|
Form |
Standard |
|---|---|
|
Metal Type |
UNS N07718 |
|
Bar |
ASTM B637 AMS 5662 AMS 5663 AMS 5664 PWA 1009 PWA 1010 GE B50TF15 |
|
Wire |
AMS 5832 |
|
Sheet |
ASTM B670 AMS 5596 AMS 5597 PWA 1033 GE B50TF14 ASTM B670 ASTM B637 |
|
Plate |
ASTM B670 AMS 5596 AMS 5597 PWA 1033 GE B50TF15 ASTM B670 ASTM B637 |
|
Tube |
AMS 5589 AMS 5590 |
|
Pipe |
AMS 5589 AMS 5590 |
|
Fitting |
|
|
Forging |
ASTM B637 AMS 5562 AMS 5663 AMS 5664 PWA 1009 PWA 1010 GE B50TF15 |
|
Weld Wire |
A5.14 ERNiFeCr-2 |
|
Weld Electrode |
|
|
Din |
2.4668 |
690 718 Inconel Alloy Pipe Specification
690 Inconel Alloy Pipe Chemical composition
| Element | Content (%) |
|---|---|
| Chromium, Cr | 27-31 |
| Iron, Fe | 7-11 |
| Silicon, Si | 0.5 max |
| Manganese, Mn | 0.5 max |
| Copper, Cu | 0.5 max |
| Silicon, Si | 0.5 max |
| Carbon, C | 0.05 max |
| Sulfur, S | 0.015 max |
| Nickel, Ni | Remainder |
718 Inconel Alloy Pipe Chemical composition
|
Element |
Percentage |
| Carbon |
0.08 max |
| Manganese |
0.35 max |
| Phosphorus |
0.015 max |
| Sulfur |
0.015 max |
| Silicon |
0.35 max |
| Chromium |
17-21 |
| Nickel |
50-55 |
| Molybdenum |
2.80-3.30 |
| Columbium |
4.75-5.50 |
| Titanium |
0.65-1.15 |
| Aluminum |
0.20-0.80 |
| Cobalt |
1.00 max |
| Boron |
0.006 max |
| Copper |
0.30 max |
| Tantalum |
0.05 max |
| Iron |
Balance |


Inconel 690 has excellent corrosion resistance against a variety of corrosive water media and high temperature environments. In addition, Inconel 690 has high strength, high metallurgical stability and excellent processing properties. The Cr in the chemical composition of the alloy makes the alloy significantly resistant to oxidizing chemicals and high-temperature oxidizing gas corrosion. The high nickel content gives the alloy resistance to stress corrosion cracking in halide-containing environments and sodium hydroxide solutions.
Alloy 718 is a precipitation-strengthened nickel-based high-temperature and high-strength alloy with good comprehensive properties in the temperature range of -253 to 700°C. The yield strength below 650°C ranks first among deformed high-temperature alloys, and has good fatigue resistance, radiation resistance, and resistance to radiation. Oxidation and corrosion resistance, as well as good processing performance, welding performance and long-term structural stability, it can manufacture various parts with complex shapes. It has been widely used in the aerospace, nuclear energy and petroleum industries in the above temperature range.
GNEE Group Factory Environment
690 718 Inconel mirror Alloy Pipe factory

690 718 Inconel Alloy Pipe process & size
690 718 Inconel Alloy Pipe process & size


Customer Case
customer visit

FAQ
Q: What are the advantages of your company?
A: We have many professionals, technicians, more competitive prices and the best after-sales service than other stainless steel companies.
Q: Can you send samples?
A: Of course, we can send samples to all over the world, our samples are free, but customers need to bear the express cost.
Q: What product information do I need to provide?
A: You need to provide the grade, width, thickness, coating and tonnage you need to purchase.
Q: About the product price of 690 718 Inconel Alloy Pipe?
A: Due to cyclical changes in raw material prices, prices vary in different periods.
Hot Tags: 690 718 inconel alloy pipe, China 690 718 inconel alloy pipe suppliers, alloy ss piping, inconel alloy sensor parts, inconel alloy resin transfer molding process, nickel-based, Inconel Pipe, inconel alloy exhaust system parts
You Might Also Like
Send Inquiry