Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of hastelloy n06455 nickel alloy in China. If you're going to wholesale high quality hastelloy n06455 nickel alloy made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Hastelloy N06455 Nickel Alloy
Properties Of Nickel Alloy Hastelloy C4
Density
Renowned for Hastelloy C4 properties, the metal stands out with a density of 8.64 g/cm3. Such a figure ensures robustness, stability, and withstands stress excellently. The lower the density, the higher the strength-to-weight ratio will be.
Melting Point
The melting point of Hastelloy C4 is notably high, precisely 1350°C. High melting points signify stronger intermolecular bonds.
Thermal Conductivity
Thermal conductivity, a crucial parameter for Hastelloy C4, is 11.5 W/m·K at 25°C. Essentially, it describes the rate at which this alloy conducts heat. High thermal conductivity materials quickly distribute heat across their surface.
Electrical Resistivity
When focusing on Hastelloy C4, the electrical resistivity stands at 1.15 μohm·m. Thus, it's not a perfect conductor of electricity. However, given its resistivity, it serves well in many corrosive environments.
Modulus Of Elasticity
The modulus of elasticity for Hastelloy C4 is 211 GPa. That's quite impressive! Such value indicates the stiffness of the material and its ability to endure and return to its original shape after stress.
Coefficient Of Expansion
For Hastelloy C4, the coefficient of thermal expansion is 11.0 μm/m°C at 20-100°C. This signifies how much the alloy will expand or contract per degree change in temperature.
Magnetic Permeability
Hastelloy C4 shows a magnetic permeability of 1.0003 at 200 oersted (15.9 kA/m). Its low magnetic response proves useful in magnetically sensitive applications.
Specific Heat
The specific heat of Hastelloy C4, also known as Hastelloy C4 2.4610, is 427 J/kg·K. In other words, it's the energy required to raise the temperature of one kilogram of the material by one degree Kelvin.
Packaging&Transportation