In order for Hastelloy C to, in a wide range of environments that can be considered severe, offer superior corrosion resistance, tungsten has been added to a nickel-molybdenum-chromium super-alloy. How does this work? To maintain resistance against corrosion in as-sprayed structures, the low carbon content, during spraying, minimizes carbide precipitation. Chromium offers resistance against oxidizing media. Especially resistant is the nickel steel alloy (with molybdenum and high nickel contents) when it comes to crevice corrosion and pitting in reducing environments. And though Hastelloy C is undeniably the most widely used, there are numerous variations of the Hastelloy nickel alloy.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of hastelloy c1 in China. If you're going to wholesale high quality hastelloy c1 made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

In order for Hastelloy C to, in a wide range of environments that can be considered severe, offer superior corrosion resistance, tungsten has been added to a nickel-molybdenum-chromium super-alloy. How does this work? To maintain resistance against corrosion in as-sprayed structures, the low carbon content, during spraying, minimizes carbide precipitation. Chromium offers resistance against oxidizing media. Especially resistant is the nickel steel alloy (with molybdenum and high nickel contents) when it comes to crevice corrosion and pitting in reducing environments. And though Hastelloy C is undeniably the most widely used, there are numerous variations of the Hastelloy nickel alloy.

Hastelloy C Ratings for Machinability

This kind of wear, temperature, cobalt, and nickel-base corrosion resistant alloy, when machining, is classified as difficult down to moderate. It is important to realize, however, that the machining of these alloys is possible at satisfactory rates using production methods which are considered conventional. These alloys harden rapidly during machining. During cutting, they generate heat and may, as a result, weld to the surface of the cutting tool. Because of their high shear strengths, they will offer high resistance to metal removal.

 

Mechanical Properties

Form Test Temperature Thickness Yield Strength
(0.2% Offset)
Tensile Strength Elongation
°F °C in mm ksi MPa ksi MPa %
Sheet RT RT 0.065 1.7 60.3 416 111.4 768 52
Sheet 400 204 0.065 1.7 58.5 403 102.4 706 49
Sheet 600 316 0.065 1.7 53.8 371 97.9 675 52
Sheet 800 427 0.065 1.7 46.4 320 95.2 656 64
Sheet RT RT 0.125 3.2 61 421 116.2 801 54
Sheet 400 204 0.125 3.2 46.4 320 98.3 678 54
Sheet 600 316 0.125 3.2 43.9 303 97.5 672 59
Sheet 800 427 0.125 3.2 43.9 303 93.4 644 62
Sheet 1000 538 0.125 3.2 43.4 299 93.5 645 55
Sheet RT RT 0.156 4 53 365 113.5 783 55
Sheet 400 204 0.156 4 39.9 275 99.9 689 55
Sheet 600 316 0.156 4 36.1 249 95.3 657 61
Sheet 800 427 0.156 4 36.2 250 95.1 656 68
Plate RT RT 0.25 6.3 48.8 336 111.3 767 58
Plate 400 204 0.25 6.3 42.8 295 104 717 54
Plate 600 316 0.25 6.3 40.8 281 103.3 712 55
Plate 800 427 0.25 6.3 37 255 99 683 60
Plate RT RT 0.375 9.5 51.6 356 114.7 791 59
Plate 400 204 0.375 9.5 43.6 301 105.4 727 56
Plate 600 316 0.375 9.5 39.1 270 102.1 704 59
Plate 800 427 0.375 9.5 37.4 258 96.3 657 62
Plate 1000 538 0.375 9.5 33 228 93.3 643 52
Plate RT RT 0.5 12.7 48.6 335 116.8 805 63
Plate 400 204 0.5 12.7 38.3 264 105.2 725 61
Plate 600 316 0.5 12.7 35.8 247 102.5 707 65
Plate 800 427 0.5 12.7 34.2 236 99.8 688 66
Plate 1000 538 0.5 12.7 29.8 205 92.1 635 71

More +

product-720-720product-720-720product-720-720product-720-720

 

 

FAQ

 

Q: How do you control quality ?
A: Mill Test Certification is supplied with shipment, Third Party Inspection is available. and we also get ISO,SGS,Alibaba Verified.
Q: What are the advantages of your company ?
A: We have many professionals, technical personnel, more competitive prices and best after-dales service than other stainless steel companies.
Q: How many coutries you already exported ?
A: Exported to more than 50 countries mainly from America, UK, Kuwait, Egypt, Turkey, Jordan,India, etc.
Q: Can you provide sample ?
A: Yes. We can provide the small samples in stock for free, as long as you contact us.Customized samples will take about 5-7 days.

Hot Tags: hastelloy c1, China hastelloy c1 suppliers, hastelloy alloy, hastelloy material piping alloy, alloy for cold working, alloy for welding, material seamless piping, alloy for distillation columns

Send Inquiry

whatsapp

Phone

E-mail

Inquiry