ASTM B705 Incoloy 825 Uns N08825 Welded Pipe
video

ASTM B705 Incoloy 825 Uns N08825 Welded Pipe

ASME SB 705 N08825 welded pipe:
Outer diameter: 6-200mm
Wall thickness: 0.35-6.00mm
ASME SB 705 welded pipe

Outer diameter: 6-200 mm
Wall thickness: 0.35-6.00 mm
Length: 0.5-12 m
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of astm b705 incoloy 825 uns n08825 welded pipe in China. If you're going to wholesale high quality astm b705 incoloy 825 uns n08825 welded pipe made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

ASTM B705 Incoloy 825 Welded Pipe

Incoloy 825 Uns N08825 Welded Pipe

ASTM B705 Incoloy 825 Uns N08825 Welded PipeASTM B705 Incoloy 825 Uns N08825 Welded Pipe

Pipes available in the market are made of various metals and alloys. Inconel is one such alloy, which is subdivided into different grades to define the properties of the product. Incoloy 825 pipes are primarily made of nickel-based alloys. 2.4858 Incoloy 825 pipe materials are designed for high strength at elevated temperatures. One of the advantages of using ASME Sb 423 UNS N08825 is that they do not require post-weld heat treatment to maintain their corrosion resistance. 825 alloy pipe suppliers recommend these pipes as they exhibit excellent corrosion resistance in a variety of phosphoric, sulfuric, and nitric acids.

ASTM B423 UNS N08825 maintains its austenitic structure even when exposed to elevated temperatures for extended periods of time. Incoloy 825 seamless pipe manufacturers design these pipes to resist both oxidizing and reducing environments, as well as sulfur-rich environments. These pipes also resist chloride ion stress corrosion cracking. ASTM B423 UNS 8825 has high tensile strength and ductility. They can operate in a wide range of temperatures from 1000 degrees Fahrenheit to cryogenic temperatures. The material used in these pipes is easily formed and welded.

UNS N08825 pipes are used in tank trucks, heat meters, electrostatic precipitator electrodes, chemical equipment, phosphoric acid evaporators, and sulfuric acid piping and containers. In addition, 825 alloy welded pipes are used in food and water hot containers, pickling tank heaters, pickling tanks, ammonium sulfate containers, expansion bellows, and ship exhaust systems. The 825 alloy clad pipes we produce are supplied to various industries in different countries. They undergo various tests to confirm their performance. Due to the low labor cost in the country, the 825 alloy seamless pipes we offer are affordable.

STM B705 UNS N08825 Incoloy 825 Welded Pipe Specification

Product Name: ASTM B705 UNS N08825 Incoloy 825 Welded Pipe

Finish: Polished, AP (Annealed & Pickled), BA (Bright & Annealed), MF

Straight lengths: Maximum 65 ft (20 m)

Forms: Straight or 'U' bent Tubes

Surface Finish:
16 micro inch Ra (ID 0.4 micron Ra) (as drawn)
4 micro inch Ra (ID 0.1 micron Ra) (electropolished)

Chemical Composition

ELEMENT INCOLOY 825
NI 38.00 – 46.00
CU 1.50 – 3.00
MO 2.50 – 3.50
FE 22.00 min
MN 1.00 max
C 0.05 max
SI 0.5 max
S 0.03 max
CR 19.50 – 23.50
AL 0.02 max
TI 0.06 – 1.20

Incoloy 825 Welded Pipe Size

OUT DIAMETER WALL THICKNESS LENGTH
NB Sizes (in stock) 1/8" ~ 8" SCH 5 / SCH 10 / SCH 40 / SCH 80 / SCH 160 Upto 6 Meters
Seamless (Custom Sizes) 5.0mm ~ 203.2mm As per requirement Upto 6 Meters
Welded (in Stock + Custom Sizes) 5.0mm ~ 1219.2mm 1.0 ~ 15.0 mm Upto 6 Meters

GNEE Group Factory Environment

ASTM B705 Uns N08825 Welded Pipe

ASTM B705 Incoloy 825 Uns N08825 Welded Pipe

GNEE Group Product Packaging

ASTM B705 Incoloy 825 Uns N08825 Pipe

ASTM B705 Incoloy 825 Uns N08825 Welded Pipe

FAQ

Q:Can we visit your factory ?
A:Warmly welcome once we have your schedule we will pick you up .
Q: Do you have quality control?
A: Yes, we have gained BV, SGS authentication.
Q: Can you arrange the shipment?
A: Sure, we have permanent freight forwarder who can gain the best price from most ship company and offer professional service.

Hot Tags: astm b705 incoloy 825 uns n08825 welded pipe, China astm b705 incoloy 825 uns n08825 welded pipe suppliers, alloy for chemical industry, hastelloy material piping alloy, alloy for aerospace, alloy for quenching, Hastelloy G 33, alloy for drawing

Send Inquiry

whatsapp

Phone

E-mail

Inquiry