Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of super duplex uns s32760 round bars in China. If you're going to wholesale high quality super duplex uns s32760 round bars made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Super Duplex UNS S32760 Round bars chemical composition are nickel, Nitrogen, molybdenum, and chromium, etc. Super Duplex UNS S32760 Round bars are mostly used for their mechanical properties and very high corrosion resistance. The high chromium and molybdenum content of Super Duplex UNS S32760 round bars make it highly resistant to corrosion by organic acid.

| Grade | C (max) | Mn (max) | Si (max) | P (max) | S (max) | Cr | Mo | Ni | N | Fe |
|---|---|---|---|---|---|---|---|---|---|---|
| S32760 | 0.05 | 1.00 | 1.00 | 0.030 | 0.010 | 24.00 – 26.00 | 3.00 – 4.00 | 6.00 – 8.00 | 0.20 – 0.30 | 57.61 (min) |
This alloy also resists inorganic acids. These round bars have some characteristics such as high strength, resistance to pitting, and stress corrosion cracking. Some other characteristics of round bars are erosion-corrosion, corrosion fatigue, and crevice corrosion. In addition, the bars have strong weldability properties. In pharmaceutical, chemical, and seawater equipment, round bars are used.

The mechanical properties of Super Duplex UNS S32760 Round bars are high tensile strength, high yield strength, density, melting point, and elongation. Stainless steel is the most versatile material; therefore, it is used in various applications. In addition, stainless steel needed very little maintenance, so it will not be changeable in very little time.