Alloy 2507 Austenitic (duplex) Stainless Steel
video

Alloy 2507 Austenitic (duplex) Stainless Steel

Item Name: Competitive price Grade 2507 Stainless steel coil Standard: ASTM,AISI,DIN,EN,GB,JIS Grade: 201,304,310S,316,316L,430,409,410 Thickness: 0.15mm-3.0mm Width: 1000mm-1500mm,or customized Edge: Slit edge/Mill edge Surface: 2B,BA,HL,Mirror,2D,No.1
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of alloy 2507 austenitic (duplex) stainless steel in China. If you're going to wholesale high quality alloy 2507 austenitic (duplex) stainless steel made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Alloy 2507 Austenitic (duplex) Stainless Steel

1.Product Description

Item Name: Competitive price Grade 2507 Stainless steel coil
Standard: ASTM,AISI,DIN,EN,GB,JIS
Grade: 201,304,310S,316,316L,430,409,410
Thickness: 0.15mm-3.0mm
Width: 1000mm-1500mm,or customized
Edge: Slit edge/Mill edge
Surface: 2B,BA,HL,Mirror,2D,No.1
Packaging: Standard exporter package or as your requirements
Origin: Foshan, China (Mainland)
Supply Ability: 5000 Tons per Month
Price terms: EX-Work,FOB,CIF,CFR,CNF
Payment terms: T/T,30%advanced payment before production and balance before shipment; OR Irrevocable L/C at sight.
MOQ: FCL, 25 metric tons per 20 GP, can be assorted with different sizes.
LCL for trial order is acceptable.
Delivery time: 10-15 days after receiving deposit by T/T or L/C.
Sample: Samples free and express charges bear by you.

Stainless steel plate/Stainless steel sheet
Grade: Stainless Steel 200 series: AISI 201, AISI 202
Stainless Steel 300 series: AISI 304, AISI 304L, AISI 316L, AISI 321, AISI 309S,AISI 310S
Stainless Steel 400 series: AISI 430, AISI 409L, AISI 443, AISI 439, AISI 441,AISI 444, AISI 436L

Chemical composition

Grade C Si Mn P S Ni Cr
AISI 201 <=0.15 <=1.00 5.5-7.5 <=0.060 <=0.03 <=3.50-5.50 <=16.00-18.00
AISI 202 <=0.15 <=1.00 7.5-10.0 <=0.060 <=0.03 <=4.0-6.0 <=17.00-19.00
AISI 304 <=0.07 <=1.00 <=2.00 <=0.045 <=0.03 <=8.00-10.5 <=18.00-20.00
AISI 316L <=0.03 <=1.00 <=2.00 <=0.045 <=0.03 <=12.00-15.00 <=16.00-18.00
AISI 309S <=0.08 <=1.00 <=2.0 <=0.045 <=0.03 <=12.00-15.00 <=22.00-24.00
AISI 310S <=0.08 <=1.00 <=2.00 <=0.045 <=0.03 <=19.00-22.00 <=24.00-26.00
AISI 321 <=0.08 <=1.00 <=2.00 <=0.045 <=0.03 <=9.00-13.00 <=17.00-19.00
AISI 409L <=0.08 <=1.00 <=1.00 <=0.045 <=0.03 <=0.50 <=10.50-17.50
AISI 430 <=0.12 <=0.75 <=1.00 <=0.040 <=0.03 <=0.60 <=16.00-18.00
AISI 436L <=0.025           <=16.00-19.00
AISI 439 <=0.03 <=1.00 <=1.00 <=0.040 <=0.03 <=0.50 <=17.00-19.00
AISI 441 <=0.015 <=1.00 <=1.00 <=0.040 <=0.03 <=0.30 <=17.50-19.00
AISI 444 <=0.025 <=1.00 <=1.00 <=0.040 <=0.03 <=1.00 <=17.50-19.50


Mechanical property

  YIELD STRENGTH TENSILE STRENGTH EXTENSION HARDNESS    
  N/mm2 N/mm2 % HRB HV HB
AISI 201 >=270 >=520 >=40 <=100 <=253 <=241
AISI 202 >=245 >=590 >=40 <=95 <=218 <=207
AISI 304 >=205 >=520 >=40 <=90 <=200 <=187
AISI 316L >=175 >=480 >=40 <=90 <=200 <=187
AISI 309S >=205 >=520 >=40 <=90 <=200 <=187
AISI 310S >= 205 >=520 >=40 <=90 <=200 <=187
AISI 321 >=205 >=520 >=40 <=90 <=200 <=187
AISI 409L >=175 >=360 >=25 <=80 <=175 <=162
AISI 430 >=205 >=450 >=22 <=88 <=200 <=183
AISI 439 >=245 >=410 >=20 <=96 <=230 <=217
AISI 441 >=302 >=495 >=35 <=96 <=170 <=217
AISI 444 >=245 >=410 >=20 <=96 <=230 <=217


Packaging & Shipping

PackagingDetails: Products are well packed and clear labeled according to the regulations and customer's requests.
Delivery Detail: 7-15days after receiving deposit

Hot Tags: alloy 2507 austenitic (duplex) stainless steel, China alloy 2507 austenitic (duplex) stainless steel suppliers, duplex stainless steel heat resistance, duplex stainless steel development, duplex stainless steel repair, duplex stainless steel estimate, duplex stainless steel bulletin, duplex stainless steel reliability

Send Inquiry

whatsapp

Phone

E-mail

Inquiry