Aluminium Alloy 7175 Plates And Sheets
video

Aluminium Alloy 7175 Plates And Sheets

Aluminium Alloy 7175 made up of high amount of aluminium, zinc, magnesium and copper. It also contains small amount of chromium. Aluminium alloy 7175 is a high strength, heat treatable, forging alloy in the wrought aluminium-magnesium family.This alloy has an combination of strength, tensile strength and stress corrosion cracking resistance.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of aluminium alloy 7175 plates and sheets in China. If you're going to wholesale high quality aluminium alloy 7175 plates and sheets made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Aluminium Alloy 7175 made up of high amount of aluminium, zinc, magnesium and copper. It also contains small amount of chromium. Aluminium alloy 7175 is a high strength, heat treatable, forging alloy in the wrought aluminium-magnesium family.This alloy has an combination of strength, tensile strength and stress corrosion cracking resistance.

4 20

Aluminium alloy 7175 sheets are best as preferred to other products as they easily get assembled and fit into machines. Their grading and preference value is also great. Aluminium Alloy 7175 sheets have great elongation capacity making them flexible for use. Their sustainability at various harmful conditions proves that they are very robust and rugged. Likewise, Aluminium alloy 7175 plates have a comfortable diameter that fits into any gadget easily and accelerates the speed of production.

Si Cr Mn Mg Cu Ti Fe Zn
0.12 0.04 0.10 1.90 – 2.60 2.00 – 2.60 0.08 – 0.21 0.15 5.70 – 6.70

219 05

 

Si Fe Cu Mn Mg Cr Zn Ti Others, each Others, total
0.10 0.12 1.2-1.9 0.06 1.9-2.6 0.18-0.25 5.2-6.2 0.06 0.05 0.15

These plates are processed using techniques like forging and heat forming. Such methods increase the hardness of the product. Aluminium alloy 7175 sheets and plates have extensive yield strength. Their resistance power is too good when it comes to matters like abrasion, erosion, etc. day and night use of these products do not hamper their usefulness. Petrochemical, pharmaceuticals, oil and gas, pulp and paper and more are some of the industries which are making use of the plates that are manufactured.

The productivity and stability of our products are maintained irrespective of many harsh environmental factors. They are even made to work at acidic media, which in turn did not affect its usability.

Hot Tags: aluminium alloy 7175 plates and sheets, China aluminium alloy 7175 plates and sheets suppliers, 5052 Aluminium Sheet Plate, 6082 T6 Aluminium Sheet Plate, Checker Aluminium Sheet Plate

Send Inquiry

whatsapp

Phone

E-mail

Inquiry