Aluminium Alloy 2011 Plates And Sheets
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of aluminium alloy 2011 plates and sheets in China. If you're going to wholesale high quality aluminium alloy 2011 plates and sheets made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Aluminium alloy 2011 is a high power alloy used at several industrial applications. It is used to manufacture automatic lathes. Manufacturing at extreme speeds produces healthy chips that are parted. The marvellous machining features permits the production of the compound and specific parts. Complete solution heat-treated and synthetically aged to T6 temper. Aluminium alloy sheets and plates2011 has erosion resistant power which helps increase its weld ability. Therefore, it is not suggested for welding. It is utilized for Fasteners, Fittings, Automotive trim.

The excellent machining features of Aluminium alloy 2011 allows the construction of complex and detailed parts. 2011 is replaced as free-machining brass without the need for alterations to tooling in certain situations. Some of the benefits of using Aluminium alloy 2011 are its more excellent corrosion resistance, Higher tensile strength, brilliant polish, High creep resistance, exceptional mechanical properties etc. Aluminium alloy 2011 can be an appropriate replacement, while higher levels of corrosion resistance are requisite. Aluminium alloy 2011 has particularly poor weldability, and therefore welding is not recommended.
Aluminium alloy 2011 sheets are the most widely used form of aluminium, is found in all of the aluminium industry's main markets. In packaging, a sheet is utilized to manufacture cans and packages. In transport, aluminium sheets are used to construct panels for automobile bodies and tractor-trailers. The excellent characteristics of the aluminium alloys sheets and plates are useful for the manufacture of complex and difficult bodies of a product. Aluminium alloy 2011 sheets and plates are used in major industrial applications such as petroleum refineries, boilers, heat exchangers, condensers etc. The aluminium alloy sheets are used widely even for manufacturing some household things too. We are producing the high-class aluminium alloys with pure quality raw materials. We offer the thermal and mechanical properties with our sheets and plates.
| Aluminium Grade | EN | WNr | UNS | DIN | BS |
|---|---|---|---|---|---|
| 2011 | AlCu6BiPb | 3.1655 | A92011 | AlCu6BiPb | FC1 |
| Chemical Composition of Aluminum 2011 Sheet and Plate | Weight (%) | Si | Fe | Cu | Pb | Bi | Zn | Al | Other |
|---|---|---|---|---|---|---|---|---|---|
| Minimum | 5.0 | 0.2 | 0.2 | 0.3 | Bal | ||||
| Maximum | 0.4 | 0.7 | 6.0 | 6.0 | 0.6 | 0.3 | Bal | 0.15 |

What is the 2011 aluminum plate used for?
2011 aluminum plate is a great choice for many needs. It has been used in the construction of a variety of structures, from vehicles to buildings. Its lightweight nature makes it easy to transport and work with. Its combination of strength and formability make it an excellent material for fabricating complex shapes and designs. Furthermore, 2011 aluminum plates corrosion-resistant properties ensure that it can maintain its structure over time. 2011 aluminum plate is truly a versatile piece of metal that can be used in a wide range of projects, from industrial and commercial applications, to artistic creations.
What are the properties of aluminium 2011 plate?
Aluminium 2011 plate is an alloy of both copper and aluminium, giving it properties of both materials. This makes it one of the most popular choices for high strength welded machined parts. It has enormous fatigue strength and relatively low weight, making it ideal for applications that require lightweight parts with good performance under cyclic loading. Its resistance to corrosion is also higher than other aluminium-copper alloys, making this material a suitable choice for parts in humid environments. Finally, its excellent electric and thermal conductivity also makes aluminium 2011 plate a great metal for radiation heat shielding applications.
Hot Tags: aluminium alloy 2011 plates and sheets, China aluminium alloy 2011 plates and sheets suppliers, 5052 Aluminium Sheet Plate, Checker Aluminium Sheet Plate, 6082 T6 Aluminium Sheet Plate