GH4080A High Temperature Alloy
video

GH4080A High Temperature Alloy

Main specifications of GH4080A
GH4080A seamless pipe, GH4080A steel plate, GH4080A round steel, GH4080A forgings, GH4080A flange, GH4080A welded pipe, GH4080A matching welding materials, GH4080A hexagonal bar, GH4080A reducer, GH4080A elbow, GH4080A tee, GH4080A bolts and nuts, GH4080A fasteners.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of gh4080a high temperature alloy in China. If you're going to wholesale high quality gh4080a high temperature alloy made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

GNEE GH4080 High temperature Alloy introduce

GH4080 High temperature Alloy

GH4080A is a NI-CR based precipitation hardening deformation high temperature alloy with a service temperature of less than 800℃. The alloy is mainly formed by adding aluminum and titanium elements to form a γ′ phase precipitation hardening phase. The alloy has good creep resistance and oxidation resistance in the range of 650-850℃. The alloy has good cold and hot processing properties. The main products are hot-rolled and forged bars, cold-drawn bars, hot-rolled plates, cold-rolled plates, strips and rings.

GNEE GH4080 High temperature Bright Bar Alloy Specification

Chemical composition of GH4080A

Alloy Element Min (%) Max (%)
GH4080A Nickel (Ni) Remainder -
  Chromium (Cr) 18 21
  Iron (Fe) - -
  Manganese (Mn) - 1.5
  Silicon (Si) - 0.4
  Phosphorus (P) - 0.02
  Sulfur (S) - 0.015
  Aluminum (Al) 1.0 1.8
  Titanium (Ti) 1.8 2.7
  Carbon (C) 0.04 0.1
  Cobalt (Co) - 2.0
  Boron (B) - 0.008
  Copper (Cu) - 0.2

GNEE GH4080 High temperature Alloy Schedule 

GH4080A Series Product Information

Product Type Products Dimensions Processes Delivery Status
Plates / Sheets Plates / Sheets 0.08-200mm (T) * W * L Forging, hot rolling, and cold rolling Annealed, Solution and Aging, Q+T, ACID WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm * L Forging, hot rolling, cold rolling, Cast Black, Rough Turning, Shot Blasting
Coil / Strip Steel Coil / Steel Strip 0.03-16.0 x 1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD: 6-219mm x WT: 0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID WASHED

GH4080 High temperature AlloyGH4080 High temperature AlloyGH4080 High temperature Alloy

 

GNEE Group Factory Environment 

GNEE Group GH4080 Alloy Factory Environment

GH4080 High temperature Bright Bar Alloy

GNEE Group Packaging 

GNEE Group GH4080 High temperature Alloy Packaging

GH4080 High temperature Bright Bar Alloy

GNEE Group Testing 

GNEE Group GH4080 Alloy Testing

GH4080 High temperature Bright Bar Alloy

FAQ

Q: What's the terms of packing?
A: Generally,we pack our goods in bundles or coils with rods or belts, we could also pack the goods as the customers' requirement.
Q: What's your delivery time?
A: For stocks, we could transport the goods to loading port within 7 work days after we received the deposit.
Q: Could you produce according to the samples?
A: Yes, we can customer-made by your samples or technique drawings, we can build the mold and fixtures.

Hot Tags: GH4080A High Temperature Alloy, China GH4080A High Temperature Alloy suppliers, Casting High Temperature Alloy