GH3536 3230 High Temperature Alloys Pipe

 

Density:8.44 g/c㎡

Melting range:1290-1350℃

Size: OD 25~320mm

W.T: 0.5 - 100mm

Length: 5.8m, 6m, 11.8m, 12m

Type: Seamless/welded

Standards:

Seamless Pipe / Tube: ASTM B444, ASTM B829, AMS 5581

Welded Pipe/tube: ASTM B705, ASTM B775, ASTM B704, ASTM B751

GH3230, a Ni-Cr-based solid solution strengthened deformed superalloy, has attracted much attention for its excellent performance over a wide temperature range (700-1050 degrees Celsius). This alloy not only has excellent high-temperature strength and thermal fatigue resistance, but also maintains excellent structural stability. GH3230 material is widely used in the manufacture of high-temperature parts such as aircraft engine barrels due to its excellent hot corrosion resistance.

Features of GH3230 material:

GH3230 superalloy exhibits excellent high-temperature strength and excellent resistance to thermal and cold fatigue. The alloy's structure remains stable, allowing it to perform well in extreme environments. In addition, the alloy also has excellent hot corrosion resistance and is suitable for long-term use in high temperature and corrosive environments.

Ingredient content of GH3230 material:

Carbon C: 0.5-0.15

Silicon Si: 0.25-0.75

ManganeseMn: 0.3-1.0

Phosphorus P: ≤0.03

Sulfur S: ≤0.015

Chromium Cr: 20-24

Nickel Ni: Yu

Molybdenum: 1-3

Lanthanum La: 0.005-0.05

CopperCu: ≤0.50

Iron: ≤3.00

NiobiumNb: ~

Boron B: ≤0.015

Titanium Ti: ≤0.10

Aluminum Al: 0.2-0.5

Vanadium V: ~

Tungsten W: 13-15

Cerium Ce: ~

Hot Tags: gh3536 3230 high temperature alloys pipe, China gh3536 3230 high temperature alloys pipe suppliers, , , ,