Stainless Steel 316 / 316L / 316Ti Sheets And Plates
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of stainless steel 316 / 316l / 316ti sheets and plates in China. If you're going to wholesale high quality stainless steel 316 / 316l / 316ti sheets and plates made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
In the same way, they are seen in the fields of marine applications because of its sober climatic adaptability and protecting attributes. This product is good to go with the different customizations concerned with its shapes, sizes, dimensions, thickness, etc. It is the last call decision of our clients. However, they all are composed of internationally accepted standards. The governing theory behind these stainless Steel is covered under the ASTM A240 and ASME SA240. They are also suitable for both the productions i.e. hot rolled and cold rolled metals.
SS 316/316L/316Ti Sheets & Plates have the maximum melting point at the 1399 degrees Celsius (or 2550 degrees Fahrenheit). They exhibit awesome tensile as well as yield strength ranges. It has the highest range of elongation at 35%. Since it belongs to the 300 families; therefore they also have the chemical make-up of carbon, manganese, silicon, phosphorus, sulphur, chromium, molybdenum, nitrogen, and nickel
.



In the same way, they are seen in the fields of marine applications because of its sober climatic adaptability and protecting attributes. This product is good to go with the different customizations concerned with its shapes, sizes, dimensions, thickness, etc. It is the last call decision of our clients. However, they all are composed of internationally accepted standards. The governing theory behind these stainless Steel is covered under the ASTM A240 and ASME SA240. They are also suitable for both the productions i.e. hot rolled and cold rolled metals.
SS 316/316L/316Ti Sheets & Plates have the maximum melting point at the 1399 degrees Celsius (or 2550 degrees Fahrenheit). They exhibit awesome tensile as well as yield strength ranges. It has the highest range of elongation at 35%. Since it belongs to the 300 families; therefore they also have the chemical make-up of carbon, manganese, silicon, phosphorus, sulphur, chromium, molybdenum, nitrogen, and nickel.
They are more often seen in the constructional as well as architectural works. For the reason that it is easily available and cost-effective in nature; it is being used in manufacturing kitchenettes like BBQ grills. They are also highly demanded in making the vessels, tanks, and storage containers in the chemical processing industries. As they consist of great stress as well as pressure tolerance attributes. Moreover, they have been utilized by the textile equipment, paper, and pulp equipment, food processing equipment industries, etc.
SS 316/316L/316Ti Sheets & Plates also present forth for the tests like PMI test, flaring test, flattening test, IGC test, etc. Other than this they provide documentations like heat treatment chart, material traceability certificates, QAP, raw material certificates, fumigation tests, etc.
316/316L/316TI STAINLESS STEEL SHEETS AND PLATES EQUIVALENT GRADES
| STANDARD | UNS | WNR. | AFNOR | EN | JIS | BS | GOST |
|---|---|---|---|---|---|---|---|
| SS 316 | S31600 | 1.4401 / 1.4436 | Z7CND17‐11‐02 | X5CrNiMo17-12-2 / X3CrNiMo17-13-3 | SUS 316 | 316S31 / 316S33 | - |
| SS 316L | S31603 | 1.4404 / 1.4435 | Z3CND17‐11‐02 / Z3CND18‐14‐03 | X2CrNiMo17-12-2 / X2CrNiMo18-14-3 | SUS 316L | 316S11 / 316S13 | 03Ch17N14M3 / 03Ch17N14M2 |
| SS 316Ti | S31635 | 1.4571 | Z2 NCDU 25-20 | X1NiCrMoCu25-20-5 | SUS 316Ti | 904S13 | - |
Stainless Steel Sheets and Plates Specification : ASTM A240 / ASME SA240
Dimension Standard : JIS, AISI, ASTM, GB, DIN, EN, etc
Width : 1000mm, 1219mm, 1500mm, 1800mm, 2000mm, 2500mm, 3000mm, 3500mm, etc
Length : 2000mm, 2440mm, 3000mm, 5800mm, 6000mm, etc
Thickness : 0.3 mm to 120 mm
Form : Coils, Foils, Rolls, Plain Sheet, Shim Sheet, Perforated Sheet, Chequered Plate, Strip, Flats, Blank (Circle), Ring (Flange) etc.
Surface Finishing : Hot rolled plate (HR), Cold rolled sheet (CR),2B, 2D, BA, NO.1, NO.4, NO.8, 8K, mirror, Chequered, embossed, hair line, sand blast, Brush, etching, SATIN (Met with Plastic Coated) etc.
Hot Tags: stainless steel 316 / 316l / 316ti sheets and plates, China stainless steel 316 / 316l / 316ti sheets and plates suppliers, ASTM A240 Grade 409L 3 0 40 0mm Hot Rolled Stainless Steel Plate, Corrugated SS Roof Sheet, SS409 Stainless Steel Welded Pipe, 1 4510 Stainless Steel Patterned Plate, Stainless Steel 316 316L 316Ti Sheets And Plates, SS431 Stainless Steel Plate