SS446 Stainless Steel Shims
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
- Tel: +8615824687445
We assure our clients of prominent manufacturing of the SS 446 Shims, and we manufactured them by utilizing the best quality material. Our products are manufactured in different forms, including the default, custom, various SS 446 Shims. The collection criteria of shims help customers go with the variation they need for their applications.

We manufacture the customized and default forms of these shims, so as per the application need, we provide the SS 446 Shims. Shims are thin portions of metal used to fill up the tiny spaces or gaps among two objects or devices. Shims can serve many purposes, including providing support, adjusting fit, or levelling out uneven surfaces.
| Grade | UNS | DIN | EN | AFNOR |
|---|---|---|---|---|
| SS 446 | S44600 | 1.4762 / 1.4763 | X10CrAlSi25 / X10CrAlSi24 | Z12CAS25 |
Chemical Composition of Stainless Steel 446 Shim:
| Grade | C (Carbon) | Mn (Manganese) | Si (Silicon) | P (Phosphorus) | S (Sulfur) | Cr (Chromium) | Mo (Molybdenum) | Ni (Nickel) | Ti + Cb |
|---|---|---|---|---|---|---|---|---|---|
| SS 446 | 0.030 max | 1.0 max | 1.0 max | 0.040 max | 0.030 max | 25.0 - 28.0 | 3.0 - 4.0 | 1.0 - 3.50 | 0.20 - 1.0 |

The manufacturing material composition of these SS 446 Shims includes the minimum amount of chromium, iron, manganese, silicon, nickel, carbon, phosphorus and sulfur. These compositions are intense, and they contain the 345MPa minimum yield strength and 550MPa minimum tensile strength. We use high-quality materials to fulfil customer's needs, requirements.
Our products have great tensile strengths and pressure capabilities to work with high-tech applications. The latest properties of our products provide the best outputs, and it works fine with critical applications also.
Hot Tags: SS446 Stainless Steel Shims, China SS446 Stainless Steel Shims suppliers, , , incoloy seamless pipe, alloy ss piping