Alloy 410S (UNS S41008) is a low carbon, non–hardening modification of Alloy 410 (UNS S41000) the general purpose 12% chromium martensitic stainless steel. The low carbon and a small alloy addition minimize austenite formation at high temperatures which restricts the alloys ability to harden. 410S remains soft and ductile even when rapidly cooled from above the critical temperature. This non-hardening characteristic helps prevent cracking when the alloy is exposed to high temperatures or welded. 410S is completely ferritic in the annealed condition. It exhibits adequate corrosion resistance similar to 410 and good oxidation resistance.

| Standard | ASTM A240, ASME SA240 |
|---|---|
| Grade | 410 |
| Thickness | 0.1mm - 100mm |
| Width | 600mm - 2500mm |
| Length | Up to 12,000mm |
| Surface Finish | No.1, 2B, No.4, HL, BA, Mirror |
| Edge Finish | Mill Edge, Slit Edge |
| Heat Treatment | Annealed, Hardened |

Cutlery
Knives and Forks: 410 stainless steel is widely used in the cutlery industry due to its ability to be hardened, providing a sharp edge and durability.
Valves and Pump Parts
Components Exposed to Corrosion and Wear: Suitable for making valves and pump parts that need moderate corrosion resistance and good wear resistance.
Automotive Parts
High Strength and Durability: Used in manufacturing various automotive parts that require robustness and resistance to wear.
Petroleum Industry
Refining and Petrochemical Applications: Ideal for parts exposed to moderate corrosive environments and requiring high strength.
Bolts, Screws, and Fasteners
Manufacturing Fasteners: Commonly used in the production of bolts, screws, and other fasteners due to its strength and corrosion resistance.
Hot Tags: alloy 410s stainless steel plate&sheet, China alloy 410s stainless steel plate&sheet suppliers, lncoloy 800H bar, high temperature alloy, Hastelloy C, Inconel alloy material, inconel alloy steel piping, high-temperature alloy
You Might Also Like
Send Inquiry