ASME SA 268 TP 410 Stainless Steel Tubing
video

ASME SA 268 TP 410 Stainless Steel Tubing

The characteristics of 410 Stainless Steel Tubing includes high tensile strength along with low fracture resistance and low ductility as well.The corrosion resistance properties of the Stainless Steel Grade 410 Round Tubing is lower in comparison to austenitic stainless steel grades. This being said, martensitic grades such as SS 410 Seamless Tubes are taken into consideration for those applications where good hardness property is a primary requirement.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

The SA 268 Gr TP 410 is a basic martensitic type of steel material that is employed as an engineering alloy. Such as most martensitic metals, UNS S41000 or Alloy Steels Grade 410 ERW Pipe can be toughened or hardened by thermal treatment.
The mechanical properties of the ASME SA 268 TP 410 Stainless Steel Tubing are improved by any heat treatment process, particularly its hardness characteristics. Compared to austenitic alloy steel standards, ASTM A268 Grade 410 Seamless Tube has inferior corrosion tolerance.As a result, martensitic standards, like A268 TP410 tubing, are considered for purposes where strong demand for hardness is present.

SEAMLESS PIPE


ASTM A268 SS Tubing Sizes Tolerance

Variations in outside diameter, wall thickness, and length from those specified shall not exceed the amounts prescribed below.

Outside Diameter, In.[Mm] OD Tolerance, In.[Mm] Wall Thickness, % Thin Wall Tubes
Up To1⁄2, [12.7], Excl ±0.005 [0.13] ±15  
1⁄2 To 11⁄2 [12.7 To 38.1], Excl/Td> ±0.005 [0.13] ±10< Less Than 0.065 In. [1.6 Mm] Nominal
11⁄2 To 31⁄2 [38.1 To 88.9], Excl ±0.010 [0.25] ±10 Less Than 0.095 In. [2.4 Mm] Nominal
31⁄2 To 51⁄2 [88.9 To 139.7], Excl ±0.015 [0.38] ±10 Less Than 0.150 In. [3.8 Mm] Nominal
51⁄2 To 8 [139.7 To 203.2], Incl ±0.030 [0.76] ±10 Less Than 0.150 In. [3.8 Mm] Nominal

 

ASTM A268 Stainless  Pipe Specification

 

Standard ASTM A268, ASME SA268
Tube Type Both Welded And Seamless
Grades ASTM A268 TP 410, ASTM A268 TP 430, ASTM A268 TP 439
Outside Diameter 1/4″ (6.25mm) To 8″ (203mm)
Wall Thickness 0.02″ (0.5mm) To 0.5″(12mm)
Application Heat Exchanger, Heater, Condenser

 

ASTM A268 TP 410 SS Tubing Mechanical Properties

Tensile Stress, Mpa Yield Stress, MPa Elongation, % Hardness, HB
415 minimum 205 minimum 20 minimum 207 maximum

 

SA 268 TP 410 Stainless Steel Tube Chemical Composition

C % Mn % P % S % Si % Cr %
0.15 maximum 1.00 maximum 0.040 maximum 0.030 maximum 1.00 maximum 11.5-13.5

 

410 Stainless Steel Equivalent

STANDARD EN / WERKSTOFF NR. UNS JIS BS AFNOR
SS 410 1.4006 S41000 SUS 410 410 S 21 Z 12 C 13

 

Customer Visit

GNEE STEEL

FAQ

Q:How should sa268 tp410 tube hardened or tempered?

A:Such as most martensitic metals, ASTM A268 TP 410 ERW tube could be hardened or tempered by heat treatment. Any heat treatment procedure applied to SA 268 TP 410 Square Tubing improves its hardness qualities and mechanical characteristics.

Q:Is a268 tp410 tubing magnetic?

A:Due to the magnetic qualities of the ASME SA268 gr 410 cold-drawn tube, which they can maintain also when annealed or heat-treated processes, as a result, ASTM a268 tp410 might be effective in operations that call for magnetism. It is always magnetic to use SA 268 TP410 pipe. The alloy's crystalline structure will determine the stainless steel's magnetic properties.

Hot Tags: asme sa 268 tp 410 stainless steel tubing, China asme sa 268 tp 410 stainless steel tubing suppliers, , monel 401 round bars, , , nickel chromium iron alloy

Send Inquiry

whatsapp

Phone

E-mail

Inquiry