General Information for Material Monel 400

Material Group S - Superalloys (Heat resistant and Titanium)
Sub-Group Superalloy
Hardness 70.0 HRB
Tensile Strength 440 [N/mm^2]
Machinability Range 45%

What is the machinability of Monel 400?What is the machinability of Monel 400?

Equivalent International Designations for Material Monel 400

UNS N04400

Standard Name
SAE 4544
WNR 2.4360
DIN NiCu30Fe
UNS
BS 3072.76
ANFOR NU30

 

Machinability of Monel 400 Material
Monel 400 is a nickel-based heat-resistant super alloy (HRSA) material with a machinability rating of 45% and a hardness of 70 HRB.

Monel 400 contains 66% nickel and other alloying elements as shown in the table below.

The main characteristics of nickel-based alloys are their excellent strength and good corrosion resistance over a wide temperature range. Within this subgroup, the material standard also defines the permissible hardness range, which is an important factor affecting machinability (in addition to chemical composition).

Monel 400 is the lowest hardness of the nickel-based alloys, so the machinability is relatively high at 45%

Superalloys should be machined with a positive sharp cutting edge. Geometries suitable for austenitic stainless steels are also suitable for HRSA. However, quality manufacturers will offer additional geometries in their catalogues that are designed specifically for these challenging materials.

Chemical Composition for Material Monel 400

Element Amount
Nickel (Ni) 66%
Silicon (Si) 0.25%
Carbon (C) 0.15%
Sulfur (S) 0.01%
Iron (Fe) 1.2%