What Are the Delivery Conditions of Inconel 718?
Inconel 718 is a precipitation-hardenable nickel-based alloy. Its delivery condition affects hardness, mechanical properties, machinability, surface finish and subsequent heat treatment. Common conditions include solution annealed, solution treated and aged, hot rolled, hot forged, cold drawn and bright annealed.
The correct condition depends on the product form, applicable material specification, component design and final application. Plate, bar, seamless tube and forgings should not automatically follow the same delivery requirements.

Heat Treatment Conditions of Inconel 718:
Heat treatment conditions determine the material's microstructure and mechanical properties. Buyers should distinguish between solution treatment and precipitation hardening before placing an order.
| Delivery Condition | Description | Main Characteristics |
|---|---|---|
| Solution Annealed | Solution heat treated | Softened condition before aging |
| Solution Treated | Solution heat treated | Prepares the alloy for subsequent precipitation hardening |
| Solution Annealed and Aged | Solution treated and subsequently aged | Higher strength after aging |
| Solution Treated and Precipitation Hardened | Solution treatment followed by precipitation hardening | Strengthened final condition |
| Age-Hardenable | Capable of precipitation hardening | Can develop higher strength through aging |
| Precipitation Hardened | Aged after solution treatment | Increased strength and hardness |
| Annealed | Heat treated to modify the material condition | Meaning depends on the applicable specification |
| Fully Annealed | Fully annealed according to a specified heat treatment | Must be defined by the purchase specification |
| Bright Annealed | Annealed in a controlled atmosphere | Bright surface with reduced oxidation and scale |
Important: Solution annealed and solution treated are often used similarly in commercial descriptions, but the exact terminology should follow the governing specification. For example, AMS 5662 covers solution heat treated Inconel 718 bars and forgings, while AMS 5663 covers solution and precipitation heat treated products.
Inconel 718 Plate Bar Tube Mechanical Processing and Surface Conditions
Hot and cold processing describe how Inconel 718 is manufactured. They are not interchangeable with final heat treatment conditions.
| Processing Condition | Product Forms | Description |
|---|---|---|
| Hot Rolled | Plate, sheet, bar | Rolled at elevated temperatures |
| Hot Finished | Bar, tube | Final dimensions achieved through hot processing |
| Hot Forged | Rings, discs, forgings | Shaped through hot forging |
| Hot Worked | Bars, billets, forgings | Deformed at elevated temperatures |
| Cold Rolled | Sheet, strip, plate | Rolled at room or near-room temperature |
| Cold Drawn | Bar, seamless tube | Drawn through dies to reduce dimensions |
| Cold Finished | Round bar, rod | Improved dimensions and surface finish through cold processing |
| Cold Worked | Bars, tubes, sheet | Strength and dimensions modified by cold deformation |
These processing routes may be followed by solution heat treatment or other specified operations. Always confirm the final delivery condition rather than relying on the processing method alone.
How to Select Inconel 718 Delivery Conditions?
Different product forms have different manufacturing and purchasing requirements.
| Product Form | Common Processing or Delivery Conditions | Applicable Specification Examples |
|---|---|---|
| Inconel 718 Plate | Solution heat treated, hot rolled, cold rolled | AMS 5596, AMS 5597, ASTM B670 |
| Inconel 718 Round Bar | Solution treated, solution treated and aged, cold finished | AMS 5662, AMS 5663, ASTM B637 |
| Inconel 718 Seamless Tube | Solution heat treated, cold drawn or hot finished as specified | AMS 5589, AMS 5590 |
| Inconel 718 Forged Ring | Hot forged, solution treated, solution treated and aged | AMS 5662, AMS 5663, ASTM B637 |
| Inconel 718 Forged Disc | Hot forged, solution treated or precipitation hardened | AMS 5662, AMS 5663, ASTM B637 |
The listed specifications are examples for the relevant product forms. Confirm the exact revision, dimensions, heat treatment and acceptance requirements before ordering.
For Inconel 718 Plate Buyers
Solution-treated Inconel 718 plate is commonly selected when the material will undergo further machining or component fabrication. Buyers should specify thickness, width, length, surface finish, flatness and required heat treatment.
For Inconel 718 Bar Buyers
Solution-treated bars are suitable when further machining and subsequent aging are planned. Solution-treated and aged bars are appropriate when the component requires specified mechanical properties in the delivered condition.
For Inconel 718 Tube Buyers
Inconel 718 seamless tubes should be selected according to outside diameter, wall thickness, length, dimensional tolerances and final heat treatment. Cold drawing and pickling may be specified as manufacturing and surface-processing requirements.
What Should Buyers Confirm Before Ordering?
Before purchasing Inconel 718 plate, bar, tube or forgings, confirm the following details:
- Material Grade: Inconel 718, UNS N07718 or the required equivalent designation.
- Product Form: Plate, sheet, round bar, seamless tube, forged ring or forged disc.
- Applicable Standard: ASTM, AMS or customer-specific specification and revision.
- Delivery Condition: Solution treated, solution treated and aged, hot finished, cold drawn or other specified condition.
- Dimensions: Thickness, diameter, wall thickness, width and length.
- Surface Requirements: Hot finished, pickled, bright annealed, polished or other specified finish.
- Inspection Documents: Chemical composition, mechanical test results, hardness and EN 10204 3.1 certificate when required.
- Packaging: Surface protection, moisture protection and export packing requirements.
Inconel 718 Products and Quotation
GNEE STEEL supplies Inconel 718 products in different forms and processing conditions, including plates, round bars, seamless tubes and forged components.
For a quotation, please provide your required product form, material specification, dimensions, delivery condition, quantity and inspection requirements. Technical drawings can also be provided for customized forged products and machining inquiries.
Contact GNEE STEEL to check available specifications, processing options and delivery arrangements for your Inconel 718 project.




FAQ:
1. Can Inconel 718 Bar Be Precipitation Hardened?
Yes. Inconel 718 is age-hardenable. A solution-treated bar can undergo precipitation heat treatment to increase strength and hardness according to the applicable specification.
2. Should Inconel 718 Forgings Use Solution and Aging?
It depends on the drawing and required mechanical properties. Solution treatment followed by aging is commonly specified for finished high-strength components. The applicable forging specification determines the acceptance requirements.
3. Can Cold Rolled Inconel 718 Sheet Have BA Finish?
A bright annealed finish can be specified when the manufacturing route and supplier capability support it. Confirm the required surface appearance, roughness and final heat treatment before ordering.
4. What Is Solution Annealed and Aged Inconel 718 Plate?
It is Inconel 718 plate that has undergone solution heat treatment followed by precipitation aging. The aging process increases strength and hardness. The final properties must meet the specified plate standard.
5. What Is Fully Annealed Inconel 718 Seamless Tube?
It refers to seamless tubing supplied after a specified annealing treatment. For Inconel 718, buyers should confirm the actual solution heat treatment requirements and applicable tubing specification rather than relying only on the term fully annealed.
6. What Is a Hot Forged Inconel 718 Forged Ring?
It is a ring-shaped component formed through hot forging. The process refines the component's shape and establishes its basic dimensions before subsequent heat treatment and machining.
7. Can Inconel 718 Bar Be Cold Finished and Bright Polished?
Yes. Cold finishing can improve dimensional accuracy and surface quality, while bright polishing provides a smoother appearance. Specify the diameter tolerance, surface roughness and polishing requirements.