Alloy 625 is a single-phase austenitic nickel-based alloy whose outstanding overall performance stems from a balanced chemistry. The high nickel (≥ 58%) and chromium (20–23%) contents provide excellent resistance to oxidation and to corrosion by reducing media; the addition of molybdenum (8–10%) significantly enhances pitting and crevice corrosion resistance; and niobium (3.15–4.15%) works synergistically with molybdenum, giving the alloy high strength through the solid-solution strengthening mechanism while stabilizing the microstructure and preventing the precipitation of harmful phases.
The alloy cannot be precipitation-hardened by heat treatment; its optimum properties are obtained through solution annealing. In the annealed condition it is essentially non-magnetic and has excellent weldability - post-weld heat treatment is usually unnecessary.
Contact us for the latest export price quote for 625 Alloy


Inconel 625 Alloy Chemical Composition
The chemical composition (weight %) of Alloy 625 is shown below; its precise control is the foundation of performance:
| Element | Content Range (min–max, %) | Primary Function |
|---|---|---|
| Nickel (Ni) | ≥ 58.0 (typically balance) | Matrix element, providing all-around corrosion resistance, high-temperature stability and immunity to chloride stress corrosion cracking |
| Chromium (Cr) | 20.0 – 23.0 | Forms a dense Cr₂O₃ oxide film, providing high-temperature oxidation resistance and resistance to oxidizing media |
| Molybdenum (Mo) | 8.0 – 10.0 | Key element, significantly improving resistance to pitting, crevice corrosion and reducing-acid attack, and providing solid-solution strengthening |
| Niobium (Nb) + Tantalum (Ta) | 3.15 – 4.15 (usually Nb-dominant) | Key strengthening element, markedly raising strength through solid-solution strengthening, stabilizing the microstructure and preventing sensitization |
| Iron (Fe) | ≤ 5.0 | Impurity element, strictly controlled |
| Carbon (C) | ≤ 0.10 | Impurity element, strictly controlled to preserve intergranular corrosion resistance |
| Manganese (Mn) | ≤ 0.50 | Deoxidizer |
| Silicon (Si) | ≤ 0.50 | Deoxidizer |
| Aluminum (Al) | ≤ 0.40 | Impurity element |
| Titanium (Ti) | ≤ 0.40 | Impurity element |
| Cobalt (Co) | ≤ 1.0 | Impurity element |
| Sulfur (S) | ≤ 0.015 | Harmful impurity, strictly controlled |
| Phosphorus (P) | ≤ 0.015 | Harmful impurity, strictly controlled |
Inconel 625 Alloy Physical Properties
| Property | Typical Value / Range | Unit | Note |
|---|---|---|---|
| Density | 8.44 | g/cm³ | Room temperature |
| Melting range | 1290 – 1350 | °C | - |
| Thermal conductivity (20–100°C) | 8.7 – 9.9 | W/(m·K) | - |
| Mean coefficient of thermal expansion (20–100°C) | 12.8 – 13.4 | ×10⁻⁶/°C | - |
| Specific heat capacity (20°C) | 394 – 427 | J/(kg·K) | - |
| Electrical resistivity (20°C) | 1.22 – 1.29 | µΩ·m | - |
| Modulus of elasticity (room temperature) | 205 – 207 | GPa | - |
| Magnetic permeability (annealed) | < 1.001 – 1.0006 | - | Essentially non-magnetic |
Inconel 625 Alloy Mechanical Properties
Room-temperature mechanical properties (solution-annealed, typical values)
| Property | Typical Value Range (min.) | Unit |
|---|---|---|
| Tensile strength (Rm) | 827 – 965 (commonly ≥ 827–930) | MPa |
| 0.2% yield strength (Rp0.2) | 414 – 517 (commonly ≥ 414–517) | MPa |
| Elongation (A) | 30 – 55% (commonly ≥ 30–42) | % |
| Hardness | 145 – 220 | HB |
High-temperature mechanical properties (short-time tensile) - Alloy 625 retains excellent strength at high temperature, with a maximum long-term service temperature of about 980°C.
| Temperature (°C) | Tensile Strength (MPa) | 0.2% Yield Strength (MPa) | Elongation (%) |
|---|---|---|---|
| 21 | 992.9 | 579.2 | 44 |
| 204 | 923.9 | 455.1 | 45 |
| 316 | 910.1 | 434.4 | 42.5 |
| 427 | 910.1 | 420.6 | 45 |
| 538 | 896.3 | 420.6 | 48 |
| 649 | 820.5 | 413.7 | 34 |
| 760 | 537.8 | 406.8 | 59 |
| 871 | 275.8 | 268.9 | 117 |
Cryogenic mechanical properties - The alloy retains excellent toughness and strength at cryogenic temperatures (e.g. liquid-nitrogen temperature, −196°C) and exhibits no ductile-to-brittle transition temperature.
Inconel 625 Alloy Key Corrosion Performance
The most outstanding feature of Alloy 625 is its exceptional all-around corrosion resistance across a wide variety of extreme corrosive environments.
| Performance Category | Description |
|---|---|
| General corrosion | Excellent resistance to oxidizing acids (e.g. nitric, phosphoric acid) and reducing acids (e.g. sulfuric, hydrochloric acid) as well as mixed acids. Performs well in hydrochloric acid of various concentrations up to 40°C. |
| Pitting and crevice corrosion | Outstanding. The high molybdenum content gives a very high pitting resistance equivalent number (PREN > 50); performance in chloride-containing environments is excellent. |
| Chloride stress corrosion cracking (SCC) | Nearly immune. The high nickel content gives the alloy extremely high resistance to chloride-induced stress corrosion cracking. |
| Seawater and marine environments | Outstanding. An ideal material for marine engineering, seawater piping, ships and offshore platforms. |
| High-temperature oxidation resistance | Excellent. Forms a stable Cr₂O₃ protective film in air up to 1100°C, with good oxidation resistance. |
| Intergranular corrosion | Good. The low carbon content and the stabilizing effect of niobium preserve good resistance to intergranular corrosion even after welding and heat treatment. |
| Environments not suitable | Corrosion resistance is excellent in strongly oxidizing media (e.g. hot concentrated nitric acid), but careful evaluation is required in certain extreme environments such as fluoride-containing media and hot concentrated alkalis. |
Inconel 625 Alloy Welding and Heat Treatment
Heat treatment:
- Stress-relief annealing - Purpose: relieve residual stress after cold working or welding. Temperature: about 899°C (1650°F), slow cooling after holding.
- Solution annealing (for optimum properties) - Purpose: dissolve carbides and obtain a uniform austenitic structure for the best corrosion resistance, ductility and strength. Temperature: 1093–1204°C (2000–2200°F), typically held at 1093–1150°C. Cooling: rapid water quench or air cooling.
Hot working: Recommended temperature range 950–1200°C (1740–2190°F). The forging finishing temperature should be kept above 900°C to avoid cracking.
Cold working: The work-hardening rate is relatively high. After cold working (e.g. cold rolling, cold drawing), intermediate annealing is required to restore ductility.
Welding:
- Weldability: Excellent - one of its principal advantages. Suitable methods include GTAW/TIG, GMAW/MIG, SMAW and SAW, among others.
- Filler metal selection: Use matched filler metals such as ERNiCrMo-3 or INCONEL® Filler Metal 625.
- Process control: Thorough cleaning before welding. Preheating and post-weld heat treatment are usually unnecessary to achieve corrosion resistance and strength comparable to the parent metal.
Inconel 625 Alloy Core Material Characteristics Summary
- Outstanding all-around corrosion resistance: excellent resistance to oxidizing/reducing acids, mixed acids, seawater and chlorides; nearly immune to chloride stress corrosion cracking, with prominent pitting and crevice corrosion resistance.
- Excellent high-temperature strength and oxidation resistance: retains good mechanical properties and oxidation resistance up to 980°C, suitable for high-temperature environments.
- Wide temperature adaptability: maintains excellent toughness and strength from cryogenic (−196°C) to high temperature (980°C), with no ductile-to-brittle transition.
- Excellent weldability: weldable by many conventional methods; post-weld heat treatment is usually unnecessary, with outstanding weld performance.
- Solid-solution strengthening, no aging: high strength through Mo and Nb solid-solution strengthening, simplifying heat-treatment procedures.
- Essentially non-magnetic: extremely low magnetic permeability in the annealed condition.
- Limitations: a pronounced tendency to work-harden - intermediate annealing is needed for cold working; use with care in extreme environments such as fluoride-containing media and hot concentrated alkalis.
Inconel 625 Alloy Application Fields
Alloy 625 is widely used in fields with extreme demands on corrosion resistance, high-temperature strength and weldability:
- Marine and offshore engineering: seawater piping systems, ship exhaust systems, offshore platform equipment, seawater desalination units, mooring chains.
- Chemical and petrochemical: reactors, heat exchangers, columns (in contact with phosphoric, sulfuric, hydrochloric acids etc.), flue gas desulfurization (FGD) systems, acid production equipment.
- Aerospace and defense: engine combustion chamber components, exhaust system ducting, thrust reversers, aircraft structural parts.
- Oil and gas: downhole tools, piping systems, flange sealing faces, burner nozzles.
- Power and energy: gas turbine components, nuclear power equipment, waste incinerator superheater tubes, geothermal power plant piping.
- Pollution control: flue gas scrubbers, absorber tower internals, high-temperature flues.
Why Choose GNEE as Your Nickel-Based Alloy Supplier?
Hastelloy Series: Hastelloy C-276, Hastelloy C-22, Hastelloy B-3, Hastelloy C-4. Mainstream materials for highly corrosive operating conditions, widely used in chemical reactors and flue gas desulfurization (FGD) units.
Inconel Nickel-Based Superalloys: Inconel 718, Inconel 625, Inconel 600, Inconel 690. Stable high-temperature strength, suitable for aerospace structural components, gas turbines, and nuclear power heat exchange equipment.
Incoloy Iron-Nickel-Based Corrosion-Resistant Alloys: Incoloy 800H, Incoloy 800HT, Incoloy 825, Incoloy 926. Combining high-temperature oxidation resistance with resistance to acid and alkali media corrosion.
Cast Nickel-Based Superalloys: Inconel 713C, Inconel 713LC. Excellent high-temperature creep and oxidation resistance, commonly used in gas turbines and turbocharger turbine castings.
Monel Alloys: Monel 400, Monel K-500. Resistant to seawater corrosion, making them common materials for marine equipment, valves, and pipe fittings.
Super Austenitic Stainless Steels: 254SMO, 904L, 654SMO. Outstanding resistance to pitting and crevice corrosion, suitable for seawater desalination and chloride-containing highly corrosive chemical environments.
Duplex Stainless Steels: 2205, 2507, S32760. High strength with excellent resistance to chloride stress corrosion cracking.
Precipitation-Hardening Stainless Steels: 17-4PH, 15-5PH, 17-7PH. High strength levels, used for precision structural components, pumps, valves, and fasteners.
Inconel 625 (UNS N06625 / W.Nr. 2.4856) Dimension Table:
| Product Form | Standard | Manufacturing Process | Size Range | Length / Unit Range | Tolerance | Delivery Condition | Surface / Finish |
|---|---|---|---|---|---|---|---|
| Heat Exchanger Seamless Tube (incl. U-bend) | ASTM B444 | Cold drawn / cold rolled | OD 4.0–50.8 mm; WT 0.5–3.5 mm | Straight ≤ 24,000 mm; U-bend per drawing | OD ±0.05 mm; WT ±10% | Solution annealed (GR.1) | Pickled / Bright Annealed (BA) |
| Seamless Pipe (process piping) | ASTM B829 / B444 | Hot extrusion + cold drawing | OD 6.0–219.1 mm; WT 0.5–20.0 mm | Fixed length ≤ 12,000 mm | Per ASTM B829 general requirements | Solution annealed | Pickled / turned / ground |
| Welded Tube | ASTM B704 | Cold rolled + continuous welding | OD 9.5–76.2 mm; WT 0.5–5.0 mm | Fixed length ≤ 12,000 mm | OD ±0.10 mm; WT ±10% | Solution annealed | Pickled / Bright Annealed |
| Welded Pipe | ASTM B705 | Welded + solution treatment | OD 25.4–323.9 mm; WT 1.65–12.7 mm | Fixed length ≤ 12,000 mm | Per ASTM B705 general requirements | Solution annealed | Pickled / polished |
| Capillary / Precision Micro Tube | ASTM B444 / B163 | Multi-pass cold drawing | OD 0.20–10.0 mm; WT 0.05–2.0 mm | Fixed length ≤ 6,000 mm; coil up to 1,000 m | OD ±0.005 to ±0.05 mm | GR.1 annealed / GR.2 stress relieved | BA / polished |
| Hot Rolled Round Bar | ASTM B446 | Hot rolled / forged | Ø6–150 mm | ≤ 6,000 mm | Per ASTM B446 general requirements | Solution / solution + aged | Black / turned / ground |
| Large Diameter Round Bar | ASTM B446 | Forged + turned | Ø160–300 mm | ≤ 4,000 mm; ≤ 1,500 kg per piece | ±0.5 mm after turning | Solution / solution + aged | Turned / ground |
| Square / Hexagonal / Flat Bar | ASTM B446 | Hot rolled / cold drawn | Square 8–200 mm; Hex 8–100 mm; Flat 3–60 mm × 10–300 mm | ≤ 6,000 mm | Per ASTM B446 general requirements | Solution / solution + aged | Pickled / turned / ground |
| Cold Drawn Wire / Welding Wire | ASTM B446 | Cold drawn | Ø0.5–12.0 mm | Coil 5–25 kg | Ø ±0.02 mm | Solution annealed / cold drawn | Bright / lubricated |
| Sheet / Cold Rolled Plate | ASTM B443 | Cold rolled | Thk 0.30–4.75 mm; W ≤ 1,219 mm | ≤ 2,438 mm; coil available | Thk ±0.05 mm (for thk ≤ 1.0 mm) | Solution annealed | 2B / pickled / brushed |
| Plate / Hot Rolled Plate | ASTM B443 | Hot rolled | Thk 4.76–100 mm; W ≤ 2,000 mm | ≤ 6,000 mm | Thk +0.3 / −0 mm and above | Solution annealed | Pickled / sheared or machined edge |
| Strip / Precision Strip | ASTM B443 | Cold rolled + slitting | Thk 0.05–0.30 mm; W 5–400 mm | Coil 50–500 kg | Thk ±0.008 mm | Solution annealed | Bright BA |
| Open Die / Closed Die Forgings | ASTM B564 | Open die / closed die forging | Max OD ≤ 1,500 mm; rings ≤ Ø1,800 mm | ≤ 1,500 kg per piece | Per drawing + machining allowance | Solution / solution + aged | Rough turned / black |
| Forged Fittings (flanges, elbows, tees, reducers) | ASTM B564 / B366 | Closed die forging + machining | DN15–DN600; flange Class 150–2500 | ≤ 800 kg per piece | Per ASME B16.5 / B16.9 | Solution + aged | Turned / weld overlay optional |
Note 1: The above sizes are normal producible ranges. Sizes beyond the upper limits require case-by-case review against billet source, machining allowance and heat treatment capability.
Note 2: ASTM B444 material is supplied in GR.1 (solution annealed) and GR.2 (stress relieved) conditions with different mechanical requirements. The condition must be stated on the order.
Note 3: For capillary tube and precision strip, OD / wall tolerance grades are classified by size. The applicable tolerance schedule is defined in the technical agreement.
Note 4: Plate and strip width / length are limited by rolling and slitting capability. Cut-to-length supply is subject to the confirmed rolling schedule.
Inconel 625 (UNS N06625 / W.Nr. 2.4856) Stock Availability Table:
| Product Form | Standard | Regular Stock Sizes (Reference) | Stock Status | MOQ | Lead Time (working days) | Remarks |
|---|---|---|---|---|---|---|
| Heat Exchanger Seamless Tube | ASTM B444 | OD 6.0–38.1 mm × WT 1.0–3.0 mm | Regular stock | 5 m | 3–7 | GR.1 / GR.2 both available |
| Seamless Pipe (process piping) | ASTM B829 | OD 25.4–114.3 mm × WT 3.0–8.0 mm | Regular stock | 1 pc | 3–7 | 6 m fixed length in stock; other lengths to schedule |
| Welded Tube | ASTM B704 | OD 12.7–50.8 mm × WT 1.0–3.0 mm | Limited stock | 10 m | 7–12 | Weld seam 100% eddy current or hydrostatic tested |
| Welded Pipe | ASTM B705 | OD 33.4–168.3 mm | Made to order | 1 pc | 20–30 | Large diameter follows welded pipe production cycle |
| Capillary / Precision Micro Tube | ASTM B444 | OD 0.5–6.0 mm × WT 0.1–1.0 mm | Limited stock | 100 m | 5–10 | Coil delivery; straight cut to length available |
| Hot Rolled Round Bar | ASTM B446 | Ø12–150 mm | Regular stock | 1 pc (≥ 1 m) | 3–7 | Black or turned finish |
| Large Diameter Round Bar | ASTM B446 | Ø160–300 mm | Made to order | 1 pc | 20–30 | Forged billet scheduling, UT included |
| Plate (6–50 mm) | ASTM B443 | Thk 6–50 mm; W 1,000–2,000 mm | Regular stock | 1 pc | 3–10 | Cutting to drawing available |
| Plate (>50–100 mm) | ASTM B443 | Thk 50–100 mm | Made to order | 1 pc | 25–35 | Heavy plate mainly rolled to order |
| Sheet / Strip | ASTM B443 | Thk 0.3–4.75 mm | Limited stock | 1 pc / 1 coil | 10–15 | Strip confirmed by coil weight and slit width |
| Forgings (flanges / rings / shafts) | ASTM B564 | Per drawing | Made to order | 1 pc | 30–45 | Drawing, NDE level and heat treatment required |
| Forged Fittings | ASTM B366 / B564 | Flanges DN15–DN200 (Class 150/300) | Limited stock | 1 pc | 10–20 | Above DN200 and high pressure classes made to order |
Note 1: Stock status is classified as Regular stock, Limited stock and Made to order. It does not represent a specific inventory quantity. Available quantity and heat number are confirmed before order placement.
Note 2: Stock sizes change with shipments. The listed sizes are regular reference ranges, not the full range of obtainable sizes.
Note 3: Lead time is normal working days after order and technical agreement confirmation, including MTC issue, excluding sea / air freight transit.
Note 4: EN 10204 3.1 MTC is supplied with each batch. 3.2 certificate, third-party witness and UT / eddy current / PMI inspection are per order agreement.




Packaging and Shipping


FAQ:
Are Alloy 625, Inconel 625 and UNS N06625 the same?
Yes - they normally refer to the same material (UNS N06625). Inconel® 625 is a registered trademark of Special Metals Corporation.
What is its maximum recommended service temperature?
Based on its oxidation resistance and high-temperature strength, the maximum long-term continuous service temperature in air or oxidizing atmospheres is 980°C (1800°F), with short-term exposure up to 1100°C (2012°F).
Why is it so resistant to chloride stress corrosion cracking (SCC)?
Its high nickel content (≥ 58%) is the fundamental reason. Nickel stabilizes the austenitic structure and greatly reduces the alloy's susceptibility to stress corrosion cracking in chloride environments, making it nearly immune.
Does it need heat treatment after welding?
Normally not. Alloy 625 has excellent weldability, and corrosion resistance and strength comparable to the parent metal are usually obtained without post-weld heat treatment. However, for thick-section weldments used under extremely severe conditions, stress-relief annealing may be advisable.
What are the main differences from Hastelloy C-276?
Alloy 625: solid-solution strengthened, focused on all-around corrosion resistance (especially chloride SCC) and high-temperature strength, with excellent weldability and no post-weld heat treatment required.
Hastelloy C-276: solid-solution strengthened, focused on extreme resistance to reducing-acid attack (e.g. hydrochloric, sulfuric acid) and local corrosion (pitting, crevice corrosion), performing better in strongly reducing environments.
What international standards does it have?
Common standards include: UNS N06625, W.Nr. 2.4856, ASTM B443 (plate/sheet), ASTM B444/B829 (seamless tube), ASTM B446 (bar), ASTM B704/B705 (welded tube), AMS 5599, AMS 5666, EN 10095, DIN 17752, etc.