GH3030 Tube Mechanical Properties At High Temperature

 
 
 
GH3030 tube mechanical properties at high temperature
GH3030 Tube Mechanical Properties At High Temperature
01.

GH3030 tube mechanical properties at high temperature

GH3030 tubing (80Ni-20Cr) is a solid solution strengthened high-temperature alloy tubing with excellent oxidation resistance and thermal stability up to 1100°C. It exhibits high plasticity and satisfactory strength below 800°C, making it an ideal material for low-load, high-temperature components such as engine combustion chambers. Furthermore, it also possesses good resistance to thermal fatigue, weldability, and corrosion resistance.

02.

What is NIMONIC 75 material?

NIMONIC 75 alloy is an 80/20 nickel-chromium alloy with added titanium and carbon. This alloy was originally introduced in the 1940s for the manufacture of turbine blades. It is easy to machine and weld, and possesses good corrosion resistance, mechanical properties, and heat resistance.

Nimonic 75 GH3030 High-Strength Nickel Alloy Tube Performance

Performance of Gnee Steel GH3030 Seamless Tubes at 800°C

When designing aerospace linings, combustion chambers, or industrial furnace components, one of the most critical challenges engineers face is structural stability. At temperatures up to 800°C (1472°F), standard alloys typically suffer from the following problems:

 

Creep deformation: Gradual elongation under sustained stress, leading to component interference.

Thermal fatigue: Cracks caused by repeated heating and cooling cycles.

Oxide scale: Material loss leading to thinning of the tube wall, reducing load-bearing capacity.

 

Our high-performance GH3030 tubes are specifically designed to address these challenges. GH3030 is a solid solution-strengthened nickel alloy that maintains its single-phase austenitic structure, ensuring industrial-grade durability even in the most demanding thermal environments.

Click to get the GH3030 tube datasheet and high-temperature test report

 

1. High-temperature tensile properties of GH3030 high-temperature alloy pipe

Understanding the "Stress-Strain" relationship at scale is vital. Below is the Technical Specification for our GH3030 seamless tubes, showing how they maintain integrity as heat increases.

Temperature (℃) Tensile Strength σb (MPa) Yield Strength σp0.2 (MPa) Elongation δ5 (%) Reduction of Area ψ (%)
20 (Room) ≥ 590 ≥ 245 ≥ 35 ≥ 40
600 (1112°F) ≥ 380 ≥ 180 ≥ 40 ≥ 45
700 (1292°F) ≥ 240 ≥ 140 ≥ 45 ≥ 55
800 (1472°F) ≥ 140 ≥ 100 ≥ 50 ≥ 60

Note: Data based on solution-treated state (1000°C-1050°C, air-cooled).

Click to download the GH3030 alloy PDF file now

 

2. Creep and Stress Fracture Properties of GH3030 Seamless Tubes

For long-term use, tensile strength alone is not enough; you also need to understand its creep resistance. GH3030 alloy is optimized for static high-temperature components where dimensional stability is critical.

Typical Stress-Rupture Life (Hours) at 800°C:

Applied Stress (MPa) Temperature (°C) Rupture Life (h) Elongation at Rupture (%)
40 800 > 100 ≥ 10
30 800 > 500 ≥ 12

By precisely controlling grain size through heat treatment, we ensure that GH3030 tubing has excellent creep resistance, preventing premature failure of critical aerospace and industrial components.

 

3. Physical properties of alloy GH3030 obtained through thermal simulation

Engineers performing finite element analysis (FEA) need accurate thermal coefficients to predict thermal expansion and heat transfer.

Property Value (at 20°C - 800°C)
Density 8.4 g/cm³
Modulus of Elasticity 158 - 200 GPa (Varies by Temp)
Mean Linear Expansion Coefficient 13.5 - 17.5 (10⁻⁶/℃)
Thermal Conductivity 14.2 - 27.2 W/(m·K)

Get Today's Wholesale Pricing for GH3030 Tubes

 

Why Choose Gnee Steel for GH3030 Steel Pipes?

As a reliable Tier 1 supplier and manufacturer, Gnee Steel offers more than just raw materials. We provide peace of mind through:

High-Purity Melting: Utilizing Vacuum Infusion Melting (VIM) + Electroslag Remelting (ESR) processes, we effectively remove impurities that cause hot cracking.

MTC 3.1 and 3.2 Traceability: Every batch undergoes rigorous high-temperature tensile testing.

Custom Processing: We offer precision cutting, bending, and special surface treatments to meet your aerospace-grade requirements.

Fast Global Logistics: With a large inventory of readily available stock, we ensure your projects proceed on schedule.

Gnee Steel GH3030 Certificate

Gnee Steel GH3030 Certificate

 

📦 Packaging and Shipping

All Nickel Based Alloy products are packaged using the following methods:

Wooden pallets or crates

Moisture-proof packaging

Labels with furnace number, standard, and size labels

Shipped worldwide by sea, air, or express

 Gnee Steel GH3030 Product Packing

 Gnee Steel GH3030 Product Packing

 

Gnee Steel
 
 

About Gnee Steel

Gnee Steel is a professional manufacturer of nickel-based alloys, including Nickel 201, Nickel 202, Hastelloy C-276, Hastelloy C-22, Hastelloy B, Hastelloy C-4, Inconel 600, Inconel 625, Inconel 718, Inconel X-750, Incoloy 800, Incoloy 800H/HT, Incoloy 825, Monel 400, Monel K500, and other high-temperature alloy materials. We specialize in the production and sales of alloy materials. Gnee Steel's products are widely used in aerospace, chemical, power generation, automotive, nuclear energy, and other fields, and we can provide customized alloy material solutions according to customer needs. For inquiries about alloy material prices or customized alloy material solutions, please feel free to contact us via email at ss@gneemetal.com for a quote.

 
35000+

Square Meters Built

 
200+

Enterprise Employees

 
18+

Years Experience

 
160+

Partner countries

Contact us for the latest export price quote for GH3030 Alloy

FAQ

Q1: How does GH3030 compare to GH3039 in terms of high-temperature strength?
A: GH3030 is a solid-solution alloy offering better plasticity and welding performance. However, for loads exceeding 850°C, GH3039 (which includes Molybdenum and Niobium) offers higher creep strength. GH3030 remains the most Cost-effective Solution for components under 800°C.

 

Q2: Can I use GH3030 tubes in a high-vibration environment at 750°C?
A: Yes. Its single-phase austenite structure provides excellent Thermal Fatigue Resistance, making it ideal for exhaust manifolds and vibrating engine parts where brittle failure must be avoided.

 

Q3: Does the welding process affect the mechanical properties?
A: When using matching filler metals (like ERNiCr-3) and proper TIG welding procedures, the joint efficiency of GH3030 is excellent. It does not require post-weld age hardening, maintaining its Structural Integrity in the as-welded state.

 

Q4: Do you provide ultrasonic testing (UT) for these tubes?
A: Absolutely. All our seamless tubes undergo 100% Eddy Current and Ultrasonic Testing to ensure zero internal defects, which is crucial for high-pressure high-temp service.