UNS N06002 Tube
video

UNS N06002 Tube

UNS N06002 pipe is a pipe made of UNS N06002 alloy, which is described as follows: Excellent corrosion resistance: UNS N06002 alloy has excellent corrosion resistance to a variety of chemical media, especially in harsh environments containing chlorides. It can resist various forms of corrosion, such as pitting, crevice corrosion and stress corrosion cracking, which makes it widely used in chemical, marine and other highly corrosive industrial environments. Good high temperature performance: The alloy maintains stable mechanical properties and corrosion resistance at high temperatures, can be used at temperatures up to 870℃, and is suitable for high temperature process equipment such as furnace components and heat exchangers. Physical properties: UNS N06002 alloy has a relatively high density (about 8.15 g/cm³) and a low thermal expansion coefficient, which makes this alloy have a small volume change when the temperature changes, which helps to maintain the stability of the structure. It has a melting point range of 1323-1371℃, has good weldability, and can be processed by various welding techniques.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of uns n06002 tube in China. If you're going to wholesale high quality uns n06002 tube made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

HASTELLOY X alloy (UNS N06002 (W86002) is a nickel-chromium-iron-molybdenum alloy that possesses an exceptional combination of oxidation resistance, fabricability and high-temperature strength. It has also been found to be exceptionally resistant to stress-corrosion cracking in petrochemical applications. X alloy exhibits good ductility after prolonged exposure at temperatures of 1200, 1400, 1600°F (650, 760 and 870°C) for 16,000 hours.

Physical Properties

Density g/cm3 8.22
lb/in.3 0.297
Melting Range °F 2300 - 2470
°C 1260 - 1355
Poisson's Ratio   0.32
Magnetic Permeability 200 oersted 1.002

Mechanical Properties

Test Temperature Yield Strength
(0.2% Offset)
Tensile Strength Elongation
°F °C ksi MPa ksi MPa %
Plate
70 21 49.3 340 110.2 760 48.9
1000 538 32.5 224 87.6 604 60.2
1200 649 30.7 212 80.9 558 63.5
1400 760 31.6 218 61 421 74.5
1600 871 27.4 189 37 255 98.1
1800 982 13.6 94 20 138 98.1
2000 1093 6.5 45 10.4 72 95.3

 

UNS N06002 pipeUNS N06002 pipeUNS N06002 pipe