Kovar Alloy Plate
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of kovar alloy plate in China. If you're going to wholesale high quality kovar alloy plate made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Kovar Alloy is a nickel-iron-cobalt alloy with a coefficient of thermal expansion like that of hard glass. Since Kovar Alloy is tough and versatile, while employing extensive quality controls throughout UNS K94610 alloy's manufacturing process to ensure uniform physical and mechanical properties for ease in deep drawing, stamping and machining are consistently achieved.
The coefficient of thermal expansion (CTE) of Kovar is its most dynamic mechanical property. It's expansion characteristics match both borosilicate (or Pyrex) glasses and alumina ceramics. This alone ensures it is a highly popular controlled expansion alloys for hermetic sealing applications (also known as Glass to Metals Sealing)
Kovar is a nickel-iron-cobalt alloy known for its low coefficient of thermal expansion (CTE). It is commonly used in applications where a tight hermetic seal between different materials is required, especially in electronic and electrical components. A Kovar capillary tube refers to a small-diameter tube made from the Kovar alloy.
The capillary tube's primary purpose is to serve as a hermetic feedthrough or a conduit for gases, liquids, or other substances in a controlled manner. The use of Kovar for capillary tubes is advantageous due to its CTE match with certain glass or ceramic materials, such as borosilicate glass or alumina, which allows for reliable sealing and prevents leaks or damage due to thermal expansion mismatch.
Kovar capillary tubes are often used in applications such as:
Glass-to-metal seals: Kovar tubes are used to provide a hermetic seal between glass and metal components, commonly found in electronic packages, vacuum tubes, and light bulbs. The Kovar capillary tube helps ensure a secure and reliable bond between the glass envelope and the metal components.
Thermal expansion control: Kovar's low CTE makes it suitable for controlling thermal expansion in various applications. By using Kovar tubes, the differential thermal expansion between different materials can be minimized, reducing the risk of stress or damage to the components.
High-reliability applications: Kovar tubes find use in high-reliability applications where precision, stability, and long-term performance are critical. Examples include aerospace, telecommunications, medical devices, and scientific instruments.
Kovar capillary tubes are typically manufactured with tight dimensional tolerances and precise internal diameters to meet specific application requirements. These tubes can be customized in terms of length, diameter, and wall thickness to suit the specific needs of the application.
It's important to note that Kovar is a trademarked name for an alloy designated as ASTM F15. When seeking Kovar capillary tubes, it's advisable to consult with manufacturers or suppliers specializing in high-quality alloys and precision components to ensure the desired specifications and performance.
Introducing our high-quality Kovar bar, meticulously engineered to meet the stringent demands of precision engineering across diverse industries. Crafted with a precise composition of approximately 29% nickel, 17% cobalt, and 53% iron, this Kovar bar embodies exceptional thermal expansion characteristics, making it an ideal choice for applications requiring a reliable hermetic seal between metal and glass.
Key Features:
Low Coefficient of Thermal Expansion (CTE): Kovar's unique blend of elements ensures a near-match with specific types of glass, maintaining stability and integrity even in extreme temperature variations.
Exceptional Durability: Engineered to withstand harsh environmental conditions while preserving its structural integrity, it ensures longevity and reliability in various applications.
Superior Machinability: Our Kovar bar is easily machinable and lends itself to precise fabrication, allowing for the creation of intricate and custom components as required by your project specifications.
Versatile Applications: Widely used in electronic and semiconductor industries for manufacturing vacuum tubes, microwave tubes, transistors, diodes, and specialized integrated circuit packages.
Why Choose Our Kovar Bar:
Reliability: Tested and proven for consistent performance, ensuring stability in critical applications.
Precision Engineering: Manufactured to exacting standards, guaranteeing uniformity and reliability across each bar.
Technical Support: Backed by our team of experts offering technical assistance and guidance to optimize the use of Kovar in your specific application.
Whether you're involved in semiconductor manufacturing, aerospace engineering, or any industry requiring precision components with dependable thermal expansion properties, our Kovar bar stands ready to meet your most demanding requirements. Invest in quality, precision, and reliability with our Kovar bar, designed to exceed your expectations and deliver exceptional performance in every application
Common Trade Names:
Kovar , NILO K, Alloy K , 4J29 , W.Nr:1.3981
Specifications:
ASTM F15 /F1466 /F29 AMS7727/ 7728 AMS I-23011 CL1
Kovar Characteristic
Reliable hermetic sealing applications
Precise and uniform thermal expansion characteristics
Their coefficient thermal expansion makes the seal resistant to shock and cracking
Kovar Chemical Composition
| % | C | P | S | Mn | Si | Cu | Cr | Mo | Ni | Co | Fe |
|---|---|---|---|---|---|---|---|---|---|---|---|
| min | - | - | - | - | - | - | - | - | 28.5 | 16.8 | - |
| max | 0.03 | 0.02 | 0.02 | 0.5 | 0.3 | 0.2 | 0.2 | 0.2 | 29.5 | 17.8 | balance |
Kovar Physical Properties
| Density | Curie Temp | Melting Point | Modulus of Elasticity at 20°C | Specific Heat | Thermal Conductivity at 20°C | Thermal Expansion | Electrical Resistivity | Poisson's coefficient |
|---|---|---|---|---|---|---|---|---|
| 8.36 g/cm³ | 435°C ( 815°F) | 1450°C (2460°F) | 207 MPa | 0.11 J/g- °C | 17.3 W/m.k | 0.17W.m-¹°C | 49 mm²/m | 0.317 |
Kovar Typical Mechanical Properties
Typical Mechanical Properties of Strip(Tested parallel to the direction of rolling,Material annealed 1830°F for 30 minutes, then furnaced cooled)
| Yield Strength,MPa | Tensile Strength,MPa | % Elongation in 2" | Hardness Rockwell B |
|---|---|---|---|
| 345 | 517 | 30 | 68 |
Magnetic Properties:
Kovar alloy is magnetic at all temperatures below the Curie point. Magnetic properties will depend upon heat treatment; the lower the hardness, the higher the permeability values and lower hysteresis loss. Examples of permeability properties are shown in the following chart:
| Flux Density | 1830°F (999°C) 30 min. - FC Permeability | 2010°F (1099°C) 20 min. - FC Permeability |
|---|---|---|
| 500 | 1000 | 1900 |
| 1000 | 1400 | 3500 |
| 2000 | 2000 | 5800 |
| 5000 | 2300 | 10000 |
| 10000 | 3400 | 8200 |
| 12000 | 3000 | 5000 |
Preparation For Sealing:
All degreased, fabricated Kovar alloy parts should be degassed and annealed in a wet hydrogen atmosphere. Atmosphere is to be made moist by bubbling the hydrogen through water at room temperature. Care must be taken to prevent surface carbon pickup. Furnace should have a cooling chamber provided with the same atmosphere. Heating should be conducted within the 1540/2010°F temperature range. Time at temperature should be approximately two hours for lowest temperature to 20 minutes for the highest temperature. Parts should then be transferred to the cooling zone and held until below 570°F, then removed. An oxide film on the metallic part is preferred for metal-to-hard glass sealing. The best oxide film is thin and tightly adhering. The film can be produced by heating the parts to 1200/1290°F in regular ambient atmosphere for a time sufficient to form a dark gray to slight brown oxide.
Kovar capillary tubes are made of a nickel-iron-cobalt alloy that has a very low thermal expansion coefficient. This makes them well-suited for applications where a close seal is required between a metal and a glass component. Kovar capillary tubes are often used in microwave devices, vacuum tubes, and other electronic components.
Properties of Kovar capillary tubes:
Material: Nickel-iron-cobalt alloy
Melting point: 1453°C (2646°F)
Tensile strength: 480 MPa (70,000 psi)
Corrosion resistance: Good
Operating temperature range: -200°C to 1250°C (-330°F to 2282°F)
Thermal expansion coefficient: 5.7 × 10^-6/°C (11.6 × 10^-6/°F)
Safety precautions for working with Kovar capillary tubes:
Wear protective clothing. This includes long sleeves, pants, gloves, and a face shield.
Work in a well-ventilated area. Kovar tubes can emit fumes that can be harmful if inhaled.
Avoid contact with the skin. If Kovar capillary tubes come into contact with your skin, wash it immediately with soap and water.
Do not weld or braze Kovar tubes in a confined space. The fumes can build up and create a dangerous environment.
Dispose of Kovar tubes properly. Do not burn or bury them, as this could release harmful fumes.
Here are some additional safety precautions that may be relevant depending on your specific work environment:
Use a fire extinguisher in case of a fire.
Have a first-aid kit on hand in case of an accident.
Train employees on the proper handling of Kovar capillary tubes.
By following these safety precautions, you can help to ensure a safe and productive work environment.
Here are some additional details about the specific safety hazards associated with Kovar capillary tubes:
Fumes: Kovar capillary tubes can emit fumes that can be harmful if inhaled. These fumes can cause respiratory problems, such as coughing, wheezing, and shortness of breath. They can also cause skin irritation and eye problems.
Fire: Kovar tubes can be easily ignited. If they come into contact with a spark or flame, they can quickly catch fire. This can be a serious hazard, as the flames can spread quickly and cause burns.
Toxicity: Kovar capillary tubes contain nickel, which is a toxic metal. If Kovar capillary tubes are ingested or inhaled, they can cause serious health problems, such as liver damage and cancer.
It is important to be aware of these safety hazards and take the necessary precautions to protect yourself when working with Kovar capillary tubes. By following the safety precautions outlined above, you can help to prevent accidents and injuries.
Kovar Available Shape
Kovar Size Range
Bars & Rods & Foring Ring /Flanges
Sheet & Plate
Strip & Coil
Welding Wire &Spring wire
Seamless Tube & Welded Pipe

Kovar ApplicationsI
Hermetic sealing
Production of transistors and diodes in electronic industry
Vacuum systems in chemistry and scientific research
Electronic tubes (power, X-Ray)
Hybrid circuit casings
Oscillator housings
Concentrated solar power
Scientific instruments
Cleaning and maintenance of Kovar capillary tubes are essential to ensure their optimal performance and longevity. Kovar, a nickel-iron-cobalt alloy, is commonly used in applications where a hermetic seal is required, such as in electronic and electrical components. Here are some guidelines for cleaning and maintaining Kovar capillary tubes:
Handling Precautions:
When handling Kovar capillary tubes, it is important to wear clean gloves to prevent contamination from oils, dirt, or moisture on the hands. This helps maintain the cleanliness of the tubes and prevents potential corrosion or surface damage.
Cleaning Procedure:
Before cleaning Kovar capillary tubes, it is advisable to refer to the manufacturer's guidelines or consult with experts familiar with the specific application. However, here is a general cleaning procedure:
a. Use a lint-free cloth or swab moistened with a mild detergent or solvent recommended for use with Kovar. Avoid using abrasive cleaners or materials that could scratch or damage the surface.
b. Gently wipe the exterior of the capillary tube, ensuring the removal of any dirt, oils, or contaminants. Take care not to apply excessive pressure that could deform or bend the tube.
c. Rinse the capillary tube with clean water or a solvent, if required, to remove any residue from the cleaning agent.
d. Dry the tube thoroughly using a clean, lint-free cloth or allow it to air-dry in a controlled environment to prevent the formation of water spots.
Storage:
Proper storage of Kovar capillary tubes is crucial to maintain their integrity. Consider the following guidelines:
a. Store the capillary tubes in a clean and dry environment to prevent exposure to moisture, which can lead to corrosion.
b. Use protective caps or covers on the ends of the tubes to prevent dust, debris, or other contaminants from entering.
c. If the capillary tubes are to be stored for an extended period, consider using desiccant packs or other humidity control measures to maintain low humidity levels.
Inspection and Maintenance:
Regular inspection of Kovar capillary tubes is recommended to identify any signs of damage, corrosion, or degradation. If any issues are detected, consult with experts or the manufacturer for appropriate maintenance or replacement procedures.
Avoidance of Harsh Environments:
Kovar capillary tubes should be used within their specified temperature and environmental limits. Exposure to extreme temperatures, corrosive chemicals, or harsh environments can adversely affect the performance and integrity of the tubes. Ensure that the capillary tubes are not subjected to conditions beyond their design capabilities.
By following these cleaning and maintenance guidelines, you can help preserve the performance and longevity of Kovar capillary tubes, ensuring their continued reliability in critical applications. It is crucial to consult with experts or refer to specific manufacturer recommendations for cleaning and maintenance procedures tailored to the unique requirements of your Kovar capillary tubes.
Feni29Co17 alloy, a blend of iron, nickel, and cobalt, represents a high-performance material renowned for its exceptional magnetic and mechanical properties. This alloy, formulated with precise ratios of its constituent elements, is tailored to meet stringent industry requirements across multiple sectors.
Key Features:
Magnetic Strength: Feni29Co17 alloy exhibits superior magnetic characteristics, making it ideal for applications requiring strong magnetism, such as in magnetic sensors, magnetic shielding, and electrical components.
Corrosion Resistance: With its excellent resistance to corrosion and oxidation, this alloy sustains its structural integrity in demanding environments, enhancing its suitability for aerospace, marine, and chemical processing applications.
Mechanical Durability: The combination of iron, nickel, and cobalt in Feni29Co17 alloy results in exceptional mechanical strength, providing durability and reliability in high-stress applications like turbine components, industrial machinery, and precision instruments.
Temperature Stability: Its stability across a wide range of temperatures makes it valuable in situations requiring consistent performance under varying thermal conditions, such as in heat exchangers or automotive applications.
Customizability: Feni29Co17 alloy can be tailored through specific heat treatments and fabrication processes to suit diverse industrial needs, allowing for a range of product variations catering to different requirements.
Applications:
Electronics and Telecommunications: Magnetic cores for transformers, inductors, and electronic components.
Aerospace and Defense: Aircraft engine parts, magnetic shielding, and aerospace components.
Energy Sector: Generators, turbines, and electrical power systems.
Medical Equipment: Magnetic resonance imaging (MRI) machines and medical diagnostic devices.
Automotive Industry: Sensors, actuators, and automotive electronic systems.
Feni29Co17 alloy stands as a testament to precision engineering, offering a versatile material solution characterized by magnetic prowess, durability, and adaptability. Its broad applicability across industries underscores its significance in modern technology and industrial advancement.
Please note that the specific properties and applications of Feni29Co17 alloy may vary based on manufacturing processes, industry standards, and intended use. For updated or more detailed information, it's advisable to consult with metallurgical experts or refer to the latest technical specifications and research in the field.
FAQ
Q: How long is your delivery time?
A: Generally it is 5-10 days if the goods are in stock. or it is 15-20 days if the goods are not in stock, it is according to quantity.
Q: Do you provide samples ? is it free or extra ?
A: Yes, we could offer the sample for free charge but do not pay the cost of freight.
Q: What is your terms of payment ?
A: Payment<=1000USD, 50% in advance. Payment>=1000USD, 30% T/T in advance ,balance before shipment.or negotiable
Hot Tags: kovar alloy plate, China kovar alloy plate suppliers, Casting High Temperature Alloy
Previous
Invar 36 Alloy PLATEYou Might Also Like
Send Inquiry