The chemical composition of 1J30 soft magnetic alloy mainly includes iron (Fe), cobalt (Co), and vanadium (V). It has the characteristics of high saturation magnetic induction intensity and low hysteresis loss, and can maintain stable magnetic properties at high frequencies.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of 1j30 6j22 precision alloy tube in China. If you're going to wholesale high quality 1j30 6j22 precision alloy tube made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

1J30 6J22 Precision Alloy Tube

Making precision resistance components: 6J22 alloy has high resistivity and temperature coefficient, so it is suitable for making precision resistance components in various measuring instruments and meters. For example, resistor sheets made of 6J22 alloy can be used to make precision measuring instruments such as resistor boxes and bridges.

Production of micro-resistance components and strain gauges: 6J22 alloy has good processing performance and mechanical properties, so it is suitable for the production of precision micro-resistance components and strain gauges. For example, micro resistors made of 6J22 alloy can be used to make micro sensors, micro electronic components, etc., while strain gauges can be used to make pressure sensors, strain measuring instruments, etc.

In addition, 6J22 alloy can also be used to make high-precision wires, springs, springs and other components, as well as high-precision instruments and equipment in aviation, aerospace, national defense and other fields.

Super Alloy Material Specification

 

Item
Brand
Chemical Composition (%)  
C S P Mn Si Ni Cr Al Fe  
1J30 ≤0.04 ≤0.020 ≤0.020 ≤0.40 ≤0.30 29.5-30.5     bal  
1J31 ≤0.04 ≤0.020 ≤0.020 ≤0.40 ≤0.30 30.5-31.5     bal  
1J32 ≤0.04 ≤0.020 ≤0.020 ≤0.40 ≤0.30 31.5-32.5     bal  
1J33 ≤0.05 ≤0.020 ≤0.020 0.30- 0.30- 32.8-33.8   1.0-2.0    
0.6 0.6 bal  
1J38 ≤0.05 ≤0.020 ≤0.020 0.30- 0.15 37.5-38.5 12.5-13.5   bal