316H Stainless Alloy Plate
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of 316h stainless alloy plate in China. If you're going to wholesale high quality 316h stainless alloy plate made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
In most instances the corrosion resistance of Alloy 316H will be comparable to Alloy 316/316 L and will have superior corrosion resistance to Alloy 304/304L. Process environments that do not attack Alloy 304/304L will not attack this grade. One exception, however, is in highly oxidizing acids such as nitric acid where stainless steels containing molybdenum are less resistant. Alloy 316H performs well in sulfur containing service such as that encountered in the pulp and paper industry. The alloy can be used in high concentrations at temperatures up to 120°F (38°C).
Alloy 316H also has good resistance to pitting in phosphoric and acetic acids. It performs well in boiling 20% phosphoric acid. The alloy can also be used in food and pharmaceutical process industries where it is utilized to handle hot organic and fatty acids where product contamination is a concern.

| Property | Value |
|---|---|
| Density | 0.285 lbs/in³ (8.00 g/cm³) |
| Electrical Resistivity | 74 Microhm-cm at 20°C (29.1 Microhm-in at 68°F) |
| Melting Range | 2507 – 2552°F (1375 – 1400°C) |
| Specific Heat | 0.11 BTU/lb-°F (32 – 212°F) (500 J/kg-°K (0 – 100°C)) |
| Modulus of Elasticity | 29.0 x 10⁶ psi (200 GPa) |
| Thermal Conductivity | 8.7 BTU/hr/ft²/ft/°F (15 W/m-°K) at 212°F (100°C) |
Alloy 316H performs well in fresh water service even with high levels of chlorides. The alloy has excellent resistance to corrosion in marine environments under atmospheric conditions.
The higher molybdenum content of Alloy 316H assures it will have superior pitting resistance to Alloy 304/304L in applications involving chloride solutions particularly in oxidizing environments.
Hot Tags: 316h stainless alloy plate, China 316h stainless alloy plate suppliers, SS409 Stainless Steel Welded Pipe, ASTM A240 Grade 431 10mm Stainless Steel Plate, ASTM A240 Grade 409L 3 0 40 0mm Hot Rolled Stainless Steel Plate, SS410 Stainless Steel Plate, 400 2 4360 Alloy Pipe, 1 4510 Stainless Steel Patterned Plate