Stainless Steel DIN1 4306 1 4307 Flanges
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
- Tel: +8615824687445
Stainless Steel DIN1.4306 1.4307 Pipe Flanges
Stainless Steel DIN1.4306 1.4307 Flanges are made from iron, chromium and nickel alloys. Chromium is the primary alloying element, giving the steel its corrosion resistance and characteristics, while nickel improves toughness and ductility. The mixture of these three chemical elements helps make this kind of stainless steel highly resistant to pitting, tarnishing and staining - perfect for any severe engineering structure or project. It is aesthetically pleasing with a glamorous sheen and durable enough to last generations.

DIN 1 4306 1 4307 SS Flanges are viral and reliable components used in the engineering and piping industries. DIN 1 4306 1 4307 stainless pipe flanges are made of austenitic stainless steel grade 304L or 304, respectively. They combine excellent corrosion-resistant properties with high temperatures, strength and hardness. Thanks to their superior quality, these durable flanges can be found in areas subject to heavy loads as well as in chemical and petrochemical applications. Furthermore, since they are prone to wear, SS DIN 1 4306 1 4307 Flanges need meagre maintenance costs and offer long-lasting service life even under harsh environmental conditions. As a result, they are an essential component of any industrial process that demands durability, reliability and superb performance at a great value.
1.4301/1.4307 X5CrNi18-10 / X2CrNi18-9, AISI 304/304L CHEMICAL COMPOSITION
| Grade | C | Si | Mn | P | S | Cr | Ni | Mo | Tio | Cu | Other |
|---|---|---|---|---|---|---|---|---|---|---|---|
| ACX 232 | <=0.030 | <=0.75 | <=2.00 | <=0.040 | <=0.030 | 18.00-20.00 | 10.00-11.00 | - | - | - | N(ppm) <700 |
Mechanical properties 1.4301/1.4307, X5CrNi18-10 / X2CrNi18-9, AISI 304/304L:
Tensile strength, Rm 460 - 700 N/mm2
Yield strength, Rp0,2: >190 N/mm2
Elongation, A: >45%
Impact strength, KV: >60J
Modulus of elasticity, E: 200 GPa
Hardness, HB: <215
Linear expansion coefficient, α: 16,0 * 10-6 K-1
Thermal capacity, cp20℃: 500 J * kg-1 * K-1
Thermal conductivity, λ: 15 W * m-1 * K-1
Resitivity, Ω: 0,73 mkOhm*m
CUSTOMER VISIT

The Group adheres to the tenet of "one-stop service, making choices easier" and adheres to the business philosophy of "successful customers, happy employees; embracing change, the most important thing is action", and continues to meet the different needs of global customers in the field of the world's steel supply chain. need. A professional sales team provides customers with first-class services; a strict procurement and quality inspection team carefully selects high-quality raw materials; an advanced science and technology team improves production and reduces costs for customers; an excellent design and processing team strives for excellence. Considerate shipping and logistics team to protect product transportation.
Hot Tags: stainless steel din1 4306 1 4307 flanges, China stainless steel din1 4306 1 4307 flanges suppliers, alloy steel tubing, , , , Hastelloy B, incoloy pipe stainless
You Might Also Like
Send Inquiry