Monel K500 Pipe Fittings
video

Monel K500 Pipe Fittings

Monel K500 Pipe Fittings are made from a nickel-copper alloy with excellent corrosion resistance and high strength. These pipe fittings are often used in marine, industrial & chemical processing applications due to their ability to resist saltwater, sulfuric acid, hydrochloric acid, alkalis & other corrosive chemicals.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Monel K500 Pipe Fittings

Product Introduction

Monel K500 Pipe Fittings provide excellent resistance to pitting, stress-corrosion cracking, erosion-corrosion, and erosive wear. These fittings have excellent ductility and toughness. Monel K500 Pipe Fittings come in various shapes, sizes, and styles. They include threaded fittings such as 90° elbows, 45° elbows, tees, crosses, couplings, end caps, and plugs. There are also butt weld fittings such as short-radius elbows, long-radius elbows, concentric reducers, eccentric reducers, and caps. There are socket-welded fittings like reducing tee's, socket-welded elbows, socket welded cross' etc., available in this material grade.

ALLOY K500 PIPES FITTING EQUIVALENT GRADE

STANDARD WERKSTOFF NR. UNS JIS BS GOST AFNOR EN
Monel K500 2.4375 N05500 - - - - -

 

MONEL K500 PIPES FITTING CHEMICAL COMPOSITION

Grade C Mn Si Cu S Ti Ni Al Fe
Monel K500 0.25 max 1.5 max 0.5 max 27.0 – 33.0 0.010 max 0.35 – 0.85 63.0 min 2.3 – 3.15 0.5 – 2

 

ALLOY K500 PIPES FITTING MECHANICAL PROPERTIES

Element Density Melting Point Tensile Strength Yield Strength (0.2%Offset) Elongation
Monel K500 8.44 g/cm3 1350 °C (2460 °F) Psi – 160000 , MPa – 1100 Psi – 115000 , MPa – 790 20 %

monel material pipe fitting

Hot Tags: monel k500 pipe fittings, China monel k500 pipe fittings suppliers, hastelloy alloy piping, high temperature corrosion resistant alloy, lnconel 718 alloy, incoloy pipe steel, incoloy material pipe seamless, nickel chromium molybdenum tungsten alloy