Cold Rolled Galvanized Steel Strip Coils Slit Edges DC01 EN 10130 / 10131 Slightly Oiled
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
- Tel: +8615824687445
Cold Rolled Galvanized Steel Strip Coils Slit Edges DC01 EN 10130 / 10131 Slightly Oiled
Description
| Width: | 600mm-1250mm | Standard: | ASTM |
|---|---|---|---|
| Length: | Coil | Grade: | Q195 DX51D DX53D SGCC |
| Technique: | Cold Rolled | Coil Weight: | 2.5-8ton |
| Type: | Steel Coil | Thickness: | 0.12-4.0 |
| Shape: | Flat.sheet,Rolled | ||
| High Light: |
Galvanized Steel Strip Coils Slit Edges,EN 10130 Steel Strip Coils,DC01 Galvanized Steel Coils |
||
Cold Rolled Steel Strip Grade DC01 According To EN 10130/10131 Slightly Oiled Slit Edges
DIN EN 10130 DC01 Steel (1.0330 Material) Data Sheet
DC01 steel (1.0330 material) is a European standard cold-rolled quality low-carbon steel flat product for cold forming. In BS and DIN EN 10130 standard, it contains 5 other steel grades: DC03 (1.0347), DC04 (1.0338), DC05 (1.0312), DC06 ( 1.0873) and DC07 (1.0898), the surface quality is divided into 2 types: DC01-A and DC01-B. In addition, this steel is also used under electrogalvanizing conditions. The designation of the steel is DC01+ZE (or 1.0330+ZE), and the standard is EN 10152.
DC01 Meaning and Definition
D: (Drawing) flat products for cold forming
C: Cold rolled
DC01: Drawing quality
DC03: Deep drawing quality;
DC04, DC05: Special deepdrawing quality;
DC06: Extra deepdrawing quality;
DC07: Super deep drawing quality.
Examples of Steel Names
DC01-A: Allow defects that do not affect formability or surface coating, such as pores, slight dents, small marks, slight scratches, and slight coloring.
DC01-B: Better surfaces shall be free from defects that may affect the uniform appearance of high-quality paints or electrolytic coatings. The other surface should meet at least surface quality A.
DC01+ZE: Electrolytically zinc coated
DC01EK: Conventionally enamelled
DC01 Steel Data Sheet
The tables and lists below give grade DC01 steel data sheet and specification including chemical composition, mechanical properties, welding, etc.
Chemical Composition
DC01 steel chemical composition is listed in the following table based on ladle analysis.
| Country (Region) | Standard | Chemical Composition (ladle analysis), %, ≤ | Surface quality | Deoxidation | Classification | ||||
| Steel name (Steel number) | C | Mn | P | S | |||||
| European Union | EN 10130 | DC01 (1.0330) | 0.12 | 0,60 | 0,045 | 0,045 | A, B | Manufacturer's discretion | Non-alloy quality steel |
| EN 10152 | DC01+ZE (1.0330+ZE) | A, B | |||||||
| EN 10139 | DC01-C390, C340, C440, C490, C590, C690 | – | |||||||
Notes:
EN 10130 – Cold rolled low carbon steel flat products;
EN 10152 – Electrolytically zinc coated cold rolled steel flat products.
EN 10139 – Cold rolled uncoated low carbon steel narrow strip.
DC01+ZE Steel Mechanical Properties
The table below lists DC01+ZE steel mechanical properties.
| Mechanical properties, Part-1 | |||||||
| Country (Region) | Standard | Steel name (Steel number) | Yield strength (MPa), 0.2 % offset | Tensile strength (MPa) | Elongation, ≥ % | Surface quality | Absence of stretcher strain marks |
| European Union | EN 10130 | DC01 (1.0330) | 140 (assumed) -280 | 270-410 | 28 | A, B | – |
| EN 10152 | DC01+ZE (1.0330+ZE) | 3 months | |||||
Notes:
Yield strength: When the thickness is ≤0.7 mm but >0.5 mm, the yield strength value should be increased by 20 MPa. For thicknesses ≤0.5 mm, the value should be increased by 40 MPa.
Elongation: When the thickness is ≤0.7 mm but >0.5 mm, the minimum value of elongation should be reduced by 2 units. For thicknesses ≤0.5 mm, the minimum value shall be reduced by 4 units.
| Mechanical properties, Part-2 | |||||||||
| Standard | Designation | Delivery condition | Symbol | Yield strength (MPa), 0.2 % offset | Tensile strength (MPa) | Elongation, A80, ≥ % | Elongation, A50, ≥ % | Hardness, HV | Validity of the mechanical properties |
| EN 10139 | DC01 (1.0330) | Annealed | A | – | 270 – 390 | 28 | 30 | ≤ 105 | 3 months |
| Skin passed | LC | ≤ 280 | 270 – 410 | 28 | 30 | ≤ 115 | |||
| Work hardened | C290 | 200 – 380 | 290 – 430 | 18 | 20 | 95-125 | |||
| C340 | ≥ 250 | 340 – 490 | Not required | Not required | 105-155 | ||||
| C390 | ≥ 310 | 390 – 540 | 117-172 | ||||||
| C440 | ≥ 360 | 440 – 590 | 135-185 | ||||||
| C490 | ≥ 420 | 490 – 640 | 155-200 | ||||||
| C590 | ≥ 520 | 590 – 740 | 185-225 | ||||||
| C690 | ≥ 630 | ≥ 690 | ≥ 215 | ||||||
Electrolytic Zinc Coatings
| Coating Designation | Nominal zinc coating values for each surface | Minimum zinc coating values for each surface | ||
| Thickness, µm | Mass, g/m² | Thickness, µm | Mass, g/m² | |
| ZE25/25 | 2,5 | 18 | 1,7 | 12 |
| ZE50/50 | 5,0 | 36 | 4,1 | 29 |
| ZE75/75 | 7,5 | 54 | 6,6 | 47 |
| ZE100/100 | 10,0 | 72 | 9,1 | 65 |
DC01+ZE Steel Mass and Density
DC01+ZE steel mass shall be calculated based on the density of steel 7.85 kg/dm³ and the density of zinc coating 7.1 kg/dm³.
Applications
The main application areas of the DC01 material include: automotive industry, construction industry, electronic equipment and home appliance industry, decorative purposes, food canning, etc.
DC01 Steel Equivalent Material
Material 1.0330, DC01 steel equivalent to ASTM, ISO, European (German DIN, British BSI, France NF), Japanese JIS and Chinese GB standard (for reference).



Hot Tags: cold rolled galvanized steel strip coils slit edges dc01 en 10130 / 10131 slightly oiled, China cold rolled galvanized steel strip coils slit edges dc01 en 10130 / 10131 slightly oiled suppliers, , , ,