Apr 08, 2025 Leave a message

Which is better C22 or C276?

Which is better C22 or C276?

 

Hastelloy C22 VS C276
Alloy C22: Hastelloy C22, UNS N06022, W.Nr.2.4602, NiCr21Mo14W
Alloy C276: Hastelloy C276, UNS N10276, W.Nr. 2.4819, NiCr16Mo15W
a) Elemental composition
Main components of C276: 57Ni-16Mo-16Cr-5Fe-4W-2.5Co-1Mn-0.35V-0.08Si-0.01C

Main components of C22: 56Ni-13Mo-22Cr-3Fe-3W-2.5Co-0.5Mn-0.35V-0.08Si-0.01C

Which is better C22 or C276?Which is better C22 or C276?

b) Welding materials
C276 welding materials: welding wire: ERnicrmo-4; welding rod: Enicrmo-4

C22 welding materials: welding wire: ERnicrmo-10; welding rod: Enicrmo-10

What we offer for Hastelloy C22 and C276
Butt welding fittings
Forged fittings
Flanges
Pipes/Tubes

Send Inquiry

whatsapp

Phone

E-mail

Inquiry