ASME SB163 MONEL 400 Nickel Alloy Air Cooler Tube
Gnee Steel
ASME SB163 MONEL 400 Nickel Alloy Air Cooler Tube
ASME SB163 Monel 400 is a nickel-copper alloy tube used in air coolers for its excellent corrosion resistance in seawater, steam, and various sour environments. Its key properties include high strength and toughness over a wide temperature range, good weldability, and resistance to chloride-ion stress corrosion cracking. It is supplied in the cold-worked condition in a variety of sizes and lengths, requiring specific fabrication methods.

Gnee Steel
What is the ASME specification for Monel 400?
Monel 400 pipe conforms to ASTM B165 and ASME SB165 international standards. Its wide variety of shapes, wall thicknesses, and sizes helps meet the specific needs of various industries, ensuring consistent quality and reliability.

Monel 400 tubing is a nickel-copper alloy known for its exceptional corrosion resistance and mechanical strength, especially in harsh environments. Alloy 400 tubing is a solid solution alloy that can only be hardened by cold working. This nickel alloy offers excellent corrosion resistance, weldability, and high strength. Its low corrosion rate in fast-moving brackish or seawater, excellent resistance to stress corrosion cracking in most freshwaters, and resistance to a wide range of corrosive conditions make it widely used in marine applications and other non-oxidizing chloride solutions. Below is a detailed overview:
ASME SB163 / B165 Monel 400 Tube Chemical Compositon:
| GRADE | C | Mn | Si | S | Cu | Fe | Ni |
| Monel 400 | 0.30Max | 2.00Max | 0.5Max | 0.24Max | 28.0-34.0 | 2.50Max | 63.00Min |
Equivalent Grades for Monel 400 Pipe Seamless Tubes:
| STANDARD | WERKSTOFF NR. | UNS | JIS | BS | GOST | AFNOR | EN |
| Monel 400 | 2.436 | N04400 | NW 4400 | NA 13 | МНЖМц 28-2,5-1,5 | NU-30M | NiCu30Fe |
ASME SB163 / B165 Monel 400 Tubing Mechanical Properties:
| Element | Density | Melting Point | Tensile Strength | Yield Strength (0.2%Offset) | Elongation |
| Monel 400 | 8.8 g/cm3 | 1350 °C (2460 °F) | Psi – 80,000 , MPa – 550 | Psi – 35,000 , MPa – 240 | 40% |
Manufacturing and Processing
Specification: ASME SB163 covers cold-worked seamless nickel and nickel alloy tubing.
Sizes: Available in a wide range of sizes, such as ½-inch to 12-inch outside diameter, with wall thicknesses from 0.8 mm to 12.7 mm, and lengths up to 26 meters.
Forming: Forming, bending (U-bends), and machining are possible, but require strict setups and specific processes to avoid work hardening.
Hardness: Available in the cold-hardened or annealed condition.
Testing and Certification
Required Testing: To ensure compliance with specifications, tubing undergoes chemical analysis, tensile testing, hydrostatic testing, and non-destructive electrical testing.
Other Testing: Other testing may include hardness, grain size, flaring, and flattening.
Certification: Material certificates, such as EN 10204 Type 3.1, are available to confirm that all specified testing has been completed.

Gnee Steel specializes in the production and sale of various nickel-based alloys, including Nickel 201, Nickel 202, Hastelloy C-276, Hastelloy C-22, Hastelloy B, Hastelloy C-4, Inconel Alloy 600, Inconel 625, Inconel 718, Inconel X-750, Incoloy Alloy 800, Incoloy 800H/HT, Incoloy 825, Monel Alloy 400, Monel K500, and high-temperature alloys. Gnee Steel's products are widely used in aerospace, chemical, electric power, automotive, and nuclear energy applications. We also offer customized alloy solutions tailored to customer needs. For alloy pricing inquiries or customized alloy solutions, please contact us for a quote at ss@gneesteel.com.