Inconel 600 Alloy Flanges
GNEE Group offers Nickel Alloy Inconel 600 in a variety of forms, including:
Bars
Wires
Sheets
Forgings
Tubes
Flanges
Seamless and Welded Pipes
Welding Rods
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of inconel 600 alloy flanges in China. If you're going to wholesale high quality inconel 600 alloy flanges made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Inconel 600 Alloy Flanges introduce
Inconel 600 Alloy Flanges


Inconel 600 flanges is manufacture from the Inconel 600, and the alloy is from the combination of nickel and chromium. Inconel 600 flanges hold on to the physical, chemical, and mechanical properties and features. These flanges are consist of materials like carbon, manganese, silicon, copper, iron, nickel, and chromium. Inconel 600 nickel chromium based alloy that offers excellent resistance to oxidation and corrosion in an environment. These flanges have higher toughness and strength in cryogenic temperature conditions.
The outstanding chemical composition of these flanges offers excellent weldability and fabricability. These Flanges are immune to chlorine ion stress-related corrosion. The Inconel alloy also shows an excellent resistance towards organic acids such as formic acid and acetic acid. The Flanges are ideal for some caustic environments. Their dimensions can be customized easily according to the exact requirements of the client.
The Inconel 600 Flanges are designed to be used in a wide range of temperatures easily. The Flanges are nickel bases in addition to chromium content that facilitates excellent durability and strength in the hostile environment. But, the nickel content facilitates excellent oxidation resistance and carburization. The flanges show oriented and acclaim sturdy construction. It shows features like corrosion-resistant, durable functioning, malleable, heat resistance, and also high strength, excellent conductivity, impeccable finish, enhanced service life, etc. Because of these excellent feature, it is used in applications like chemical plants, gas and water pipeline, industrial machinery, petroleum refining, power generation, thermal nuclear and solar power plants, petrochemical and refineries, oil and gas exploration, etc. The specification of flanges covers nickel alloy flanges. These alloys are categorized into different grades according to their chemical composition.
Inconel 600 Flanges Specifications
| Product Name: | Inconel 600 Flanges |
| Specifications: | ASTM B564 / ASME SB564 |
| size: | 1/2″ (15 NB) to 48″ (1200NB) DN10~DN5000 |
| Dimensions: | ANSI B16.5, ANSI B16.47 Series A & B, MSS SP44, ASA, API-605, AWWA, Custom Drawings |
| Standard: | ANSI Flanges, ASME Flanges, BS Flanges, DIN Flanges, EN Flanges etc. |
| Pressure Class: | Class 150 LBS, 300 LBS, 400 LBS, 600 LBS, 900 LBS, 1500 LBS, 2500 LBS | PN6, PN10, PN16, PN25, PN40, PN64 etc. |
| Coating: | Anti-rust Paint, Oil Black Paint, Yellow Transparent, Zinc Plated, Cold and Hot Dip Galvanized |
| common types: | Forged / Screwed / Threaded / Plate |
| Test Certificates: | Third Party Inspection Report, 100% Radiography Test Report, Raw Materials Certificate, EN 10204/3.1B, etc. |
| Flange Face Type: | Raised Face (RF), Flat Face (FF), Ring Type Joint (RTJ), Large Male-Female (LMF), Small Male-Female (SMF), Lap-Joint Face (LJF), Large Tongue & Groove (T&G). |
| Test Certificates (TC): | Raw Materials Certificate, EN 10204/3.1B, 100% Radiography Test Report, Third Party Inspection Report, etc |
| Material Test Certificates (MTC): | As per EN 10204 3.1 and EN 10204 3.2, TC certifying NACE MR0103, NACE MR0175 |
| Uses & Applications: | Petrochemicals and acids, Nuclear Power, Heavy oil refineries, Bitumen upgraders. |
ASTM B564 Inconel 600 Flanges Equivalent Grades
| STANDARD | UNS | WERKSTOFF NR. | AFNOR | EN | JIS | BS | GOST | OR |
| Inconel 600 | N06600 | 2.4816 | NC15FE11M | NiCr15Fe | NCF 600 | NA 13 | МНЖМц 28-2,5-1,5 | ЭИ868 |
Inconel 600 Flanges Chemical Composition
| Grade | C | Mn | Si | S | Cu | Fe | Ni | Cr |
| 600 | 0.15 | 1.00 | 0.50 | 0.015 | 0.50 | 6.00 – 10.0 | 72.00 | 14.00 – 17.00 |
Alloy 600 Flanges Mechanical Properties
| Grade | Density | Melting Point | Yield Strength (0.2%Offset) | Tensile Strength | Elongation |
| 600 | 8.47 g/cm3 | 1413 °C (2580 °F) | Psi – 45,000 , MPa – 310 | Psi – 95,000 , MPa -655 | 40 % |
Inconel 600 Flanges Size Range
| Below Mentioned Alloy 600 Flanges Size: 1/8″ – 36″ | |
| ASTM B564 Inconel 600 Slip-On Flanges | ASTM B564 Inconel 600 Threaded Flanges |
| ASTM B564 Inconel 600 Lap Joint Flanges | ASTM B564 Inconel Alloy 600 Plate Flanges |
| ASTM B564 Inconel 600 Weld Neck Flanges | ASTM B564 Inconel 600 Socket Weld Flanges |
| ASTM B564 Alloy 600 Blind Flanges | ASTM B564 Inconel 600 Reducing Flanges |
| ASTM B564 Inconel 600 Ring Type Joint Flanges | ASTM B564 Inconel Alloy 600 Square Flanges |
| ASTM B564 Inconel 600 Orifice Flanges | ASTM B564 Inconel 600 Forged Flanges |
GNEE Group Product Testing
Inconel 600 Alloy Flanges

GNEE Group Product Packaging
Inconel 600 Alloy Flanges


FAQ
Q:Can we visit your factory ?
A:Warmly welcome once we have your schedule we will pick you up .
Q: Do you have quality control?
A: Yes, we have gained BV, SGS authentication.
Q: Can you arrange the shipment?
A: Sure, we have permanent freight forwarder who can gain the best price from most ship company and offer professional service.
Hot Tags: inconel 600 alloy flanges, China inconel 600 alloy flanges suppliers, inconel alloy detector parts, nickel-based, Inconel 713C 625 Pipe, inconel alloy filter parts, inconel alloy transmitter parts, inconel alloy reducer fittings
You Might Also Like
Send Inquiry