Inconel X-750 Alloy Flanges
video

Inconel X-750 Alloy Flanges

Available Formats
GNEE Group offers Nickel Alloy Inconel X-750 in a variety of forms, including:
Bars
Sheets
Forgings
Tubes
Flanges
Seamless and Welded Pipes
Welding Rods
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of inconel x-750 alloy flanges in China. If you're going to wholesale high quality inconel x-750 alloy flanges made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Inconel X-750 Alloy Flanges introduce

Inconel X-750 Flanges

Inconel X-750 Alloy FlangesInconel X-750 Alloy Flanges

GNEE Steel is one of the leading suppliers and exporters of Inconel X-750, offering high quality Inconel x-750 flanges that can be used as backing for a variety of different purposes. A highly acclaimed supplier of Inconel X-750 Flanges, Inconel X-750 Weld Neck Flanges, Inconel X-750 Slip On Flanges, Inconel X-750 Blind Flanges. Inconel Alloy X-750 is a nickel-chromium austenitic alloy similar to Alloy 600 but made precipitation hardenable by the addition of Aluminium and Titanium. Inconel X750 has excellent resistance to relaxation and hence is used in springs that work at elevated temperatures. Alloy X750 is a precipitation hardening austenitic nickel-chromium alloy.

GNEE Steel offers X-750 flanges at very reasonable prices. We manufacture Inconel X-750 pipe flanges using high quality material. Supplying ASTM B564 Alloy X-750 Ring Joint Flanges at reasonable cost. Inconel X750 flange rings manufactured by GNEE Steel offer corrosion resistance, high temperature resistance and ultimate tensile strength. Inconel x-750 flanges have excellent mechanical properties and provide good oxidation resistance.

Inconel alloy X-750 is a precipitation hardening alloy that has been used in applications like high temperature structural members. The stress corrosion cracking (SCC) behavior of Inconel X-750 in high temperature water has been examined based on aging conditions. We specialize in supplying high nickel alloy inconel x750 raw material in India, especially for high strength and high temperature industries. Inconel X750 is resistant to a wide range of industrial corrosive agents and is both oxidizing and reducing at high temperatures.

Standards Specification of X-750 Flanges

Specifications ASTM B564 / ASME SB564 / SB160 / SB472 / SB162
Material Inconel X-750 (UNS No. N07750)
Dimension ANSI B16.5, ANSI B16.47 Series A & B, MSS SP44, ASA, API-605, AWWA, Custom Drawings
Standard ANSI Flanges, ASME Flanges, BS Flanges, DIN Flanges, EN Flanges, etc.
Size 1/2" (15 NB) to 48" (1200NB)
BS BS4504 , BS4504, BS1560, BS10.
DIN DIN2527, DIN2566, DIN2573, DIN2576, DIN2641, DIN2642, DIN2655, DIN2656, DIN2627, DIN2628, DIN2629, DIN 2631, DIN2632, DIN2633, DIN2634, DIN2635, DIN2636,DIN2637, DIN2638, DIN2673
Class 150 LBS, 300 LBS, 600 LBS, 900 LBS, 1500 LBS, 2500 LBS, DIN Standard ND-6,10, 16, 25, 40 Etc.
Flange Face Type Flate Face (FF), Raised Face (RF), Ring Type Joint (RTJ)

X-750 Alloy Flange Forms & Availability

Size Products
Sizes 1/8″ – 36″
Raised Face or Flat Face
Alloy X-750 BS 10 Table D Flange Manufacturer in Mumbai Nickel Alloy X-750 Plate Flange
Inconel X-750 Flanges Manufacturer Inconel X50 Flanges Supplier
Inconel X-750 Flanges Stockist Alloy X-750 BS 10 Table E Flanges
X-750 Inconel BS 10 Table F Flanges Manufacturer ASTM B564 Alloy X-750 Reducing Flanges
X-750 Inconel Slip On Plate Flange Nickel Alloy X-750 Plate Flanges

GNEE Group Factory Environment

Inconel  Alloy Flanges

Inconel  Alloy Flanges

Inconel X-750 Alloy Flanges

FAQ

Q1: How can we get the sample?

A1: Free samples are available for your checking and testing.But you need to pay for the frieght cost.

Q2: Can you provide Mill Test Certificate?

A2: Yes! The Mill Test Certificate will be issued with the product.

Q3:Packing details?

A3:Packaged 25 Tons per 20 GP wooden case container.

20ft GP: 5898mm(Length)x2352mm(Width)x2393mm(High)

40ft GP:12032mm(Length)x2352mm(Width)x2393mm(High)

40ft HC: 12032mm(Lengh)x2352mm(Width)x2698mm(High)

Q4:What is your terms of payment?

A4: 100% T/T advance.

30% T/T and balance against copy of documents.

30% T/T advance, balance L/C at sight.

Q5:Can we visit your factory?

A5: Warmly welcome. Once we have your schedule, we will arrange the professional sales team to follow up your case.

Hot Tags: inconel x-750 alloy flanges, China inconel x-750 alloy flanges suppliers, inconel alloy radar system parts, inconel alloy intake system parts, Inconel Weld Neck Flanges, inconel alloy connecting rod parts, lnconel 601 round bar, inconel alloy resonator parts

Send Inquiry

whatsapp

Phone

E-mail

Inquiry